MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Fibre Glast 173 Clear Gel Coat  (discontinued **)
Categories: Polymer; Thermoset

Material Notes: #173 is the highest quality gel coat from Fibre Glast. It is fully UV resistant so it may be used as a protective clear coat over other colors or glitterflake. Very true color reproduction can be achieved when mixing with color pigments. Blend with Hi-Gloss Additive when top coating. #173 is specifically formulated to be used in applications where an exterior clear gel coat is required. Examples include metal flake or clear coat backed with a solid color. #173 yields good exterior durability, flexibility, spray ability, color and clarity and is acceptable for marine applications.
  • 49-51% Volatile Organic Compounds
  • 45-60 minute lay-up time
  • Good sag resistance at 20 mils

#173 is formulated for airless, air-assist airless and conventional spray application. Brushing or rolling is not recommended.

Information provided by Fibre Glast Developments Corporation.

Vendors:
Available Properties
  • Brookfield Viscosity, Brookfield RVF #4 Spindle at 20 rpm
  • Flash Point
  • Transmission, Visible, clear; thickness not quantified
  • Gel Time, Value at 77°F with 1.8% MEKP
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Fibre Glast Developments Corporation

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.