MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Arkema Oroglas® V 825 HID Acrylic, UV, Heat Resistant  (discontinued **)
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, UV Stabilized, Molded

Material Notes: OROGLAS HID is an acrylic resin formulated to withstand continuous exposure to high intensity discharge ( HID ) sources up to 90°c.

Above 80°c, OROGLAS V 825 HID resin retains its original appearance while other plastics typically used in HID lighting yellow.

OROGLAS V 825 HID is specifically designed to be used at the highest acrylic UL relative thermal index, 90°c.

The excellent balance of mechanical, thermal and optical properties are the same as OROGLAS V 825 T resins.

When applications require stability to intense UV light at temperatures above 80°c, OROGLAS V 825 HID deliver superior long term performance. Typically the most demanding lighting applications use high intensity discharge sources.

OROGLAS V 825 HID can be used in any lighting application. It may be a wise choice for certain compact fluorescent or incandescent fixtures where the lens is close to the lamp.

OROGLAS V 825 HID is recognized under all UL component listings and carries a 90°c RTI, the highest o

Vendors:
Available Properties
  • Density
  • Water Absorption
  • Moisture Absorption at Equilibrium, Humidity Absorption
  • Melt Flow
  • Tensile Strength, Yield, 50 mm/min
  • Elongation at Break, Nominal Strain; 50 mm/min
  • Tensile Modulus, 1 mm/min
  • Charpy Impact Unnotched
  • Charpy Impact, Notched
  • Tensile Creep Modulus, 1 hour
  • Tensile Creep Modulus, 1000 hours
  • Electrical Resistivity
  • Surface Resistance
  • Dielectric Constant
  • Dielectric Constant
  • Dielectric Strength
  • Dissipation Factor
  • Dissipation Factor
  • Comparative Tracking Index
  • CTE, linear, Parallel to Flow
  • Maximum Service Temperature, Air
  • Deflection Temperature at 0.46 MPa (66 psi)
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Vicat Softening Point, 50°C/hr; 50N
  • Flammability, UL94
  • Transmission, Visible, Mfr. reports 'Transparent' but doesn't quantify.
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Arkema Group

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.