MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Syensqo (Solvay Specialty Polymers) Algoflon® F 5 PTFE, Powder
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE); Polytetrafluoroethylene (PTFE), Bronze Filled

Material Notes: Algoflon® F 5 is a fine cut homopolymer PTFE powder that is white, granular and non-free flowing. It is designed for filled grades and in particular is recommended for compounds with glass fiber since it allows good degassing during the sintering process.

Main features of Algoflon® F 5 are:

- Fine particle size
- Narrow particle size distribution
- Good blendability
- Low porosity

Applications: Additive; Blending

Features: Chemical Resistant

Processing
- Algoflon® F 5 is used for preparing filled products based on PTFE resins. Prior to use, Algoflon® F 5 powder needs to be conditioned above 19°C/66°F.
- In order to obtain fully homogeneous compounds, it is necessary to mix Algoflon® F 5 and filler with high shear systems. Temperature must also be controlled (it should not rise above 40°C/104°F) during the mixing process to avoid agglomeration of PTFE and generation of white spots.
- Algoflon® F 5 based compounds are processed using normal compression molding as similar to virgin fine cut PTFE.

Storage and Handling
- Algoflon® PTFE fine cut powders must be stored and handled carefully to achieve defect free molding. Before use the temperature of the powder must be conditioned above 19 °C / 66 °F (between 21-27 °C / 70–81 °F). Below this temperature, the powder is difficult to mold without cracks. Too high temperatures should also be avoided to prevent powder lumping and poor flow.
- Storage and handling facilities should be clean since even very small foreign particles can cause defects in finished products. Keep resin drums closed and clean. Good housekeeping and careful handling are essential.
- Each drum contains two bags liner made of polyethylene resin. The external bag liner is used only to protect the PTFE powders against external contamination. It is recommended to remove and isolate the external liner before handling and opening the internal layer which is in contact with the PTFE powders.

Safety and Toxicology
- Before using Algoflon® PTFE fine cut powders, consult the product Material Safety Data Sheet and follow all label directions and handling precautions.
- As with all PTFE materials, handling and processing should only be carried out in well ventilated areas. Vapor extractor units should be installed above processing equipment. Fumes must not be inhaled and eye and skin contact ought to be avoided. In case of skin contact wash with soap and water. In case of eye contact flush with water immediately and seek medical help.
- Do not smoke in areas contaminated with powder, vapor or fumes.

Information provided by Solvay Specialty Polymers.

Vendors:
Available Properties
  • Specific Gravity, ASTM D792
  • Bulk Density, ASTM D4894
  • Particle Size, Average
  • Tensile Strength, ASTM D4894
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Solvay Specialty Polymers (includes former Solexis)

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.