MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Empilon EMPILON® 770 TPE
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: EMPILON® series can be widely used in general products (such as tool grips, automotive parts, industrial products, sporting goods, etc.) that require high tensile strength, heat resistance and weather resistance. It is mainly a hydrogenated Styrenic Block Copolymer blending materials, hardness range from Shore A16 to Shore D52, can be processed by injection molding, extrusion molding and calendaring. The series is non-toxic. It does not contain RCRA 8 heavy metals, halogens, phthalate and is 100% recyclable and eco-friendly. It can pass the European Union Waste Electronics and Electrical Equipment (WEEE), Restriction of Hazardous Substances (RoHS) regulations and meet the environmental requirements of SONY SS-00259 4th Edition. The series has good chemical resistant and hydrolysis resistant performance.This series can be used without drying before processing. If you want to dye this series of products, please choose PE or EVA as the substrate of masterbatch, never use PVC as the substrate. Moreover, use a higher screw speed when processing and higher back pressure to achieve better dispersion of the colorant.

Series Features:

  • Excellent Mechanical Property and Toughness
  • Excellent Weather Resistance
  • Excellent Heat Aging Resistance
  • Excellent Low Temperature Property
  • Chemical Resistance
  • Hydrolysis Resistance
  • Easy to Processing, apply to general usage product
  • Wide Hardness Range
  • Apply to weather resistant and high strength product
  • Apply to sporting and industrial goods
Applications:
  • Derailleur Cap: Escalate quality
  • Bike Pedals: Aesthetic/Comfortable tactile feeling
  • Scissors Handle: Aesthetic/Comfortable tactile feeling
  • Toy Car Wheel: Comfortable tactile feeling/Wear resistance
  • Comfortable tactile: Comfortable tactile feeling/Good sealing performance
  • Fins: Hydrolysis Resistance/Comfortable tactile feeling

Information provided by EMILON®

Vendors:
Available Properties
  • Specific Gravity, ASTM D792
  • Melt Flow, ASTM D1238
  • Hardness, Shore A, ASTM D2240
  • Tensile Strength, ASTM D412
  • Elongation at Break, ASTM D412
  • Brittleness Temperature
  • Shrinkage, MD
  • Shrinkage, TD
  • Feed Temperature
  • Middle Barrel Temperature
  • Front Barrel Temperature
  • Nozzle Temperature
  • Melt Temperature
  • Melt Temperature, do not exceed
  • Mold Temperature
  • Injection Pressure
  • Back Pressure
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic
Thermoplastic Elastomer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.