MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Eastman AP005 Copolyester  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: Applications:
  • Automotive components
  • Breathable films
  • Electrical/electronic components
  • Film Modification
  • Flexible hinges
  • Hose mandrel
  • Industrial components
  • Industrial hoses/belts
  • Office furniture
  • Packaging
  • Polymer modification
  • Profiles
  • Rubber and plastic modification
  • Sporting goods
  • Thermoplastic elastomer compounds
  • Tubing

Key Attributes:

  • Environmentally preferred, non-halogenated material
  • Excellent chemical and oil resistance
  • Excellent compatibility with a wide range of polymers
  • Excellent processability
  • Exceptional heat resistance and high temperature dimensional stability
  • High energy absorption
  • High flexibility without plasticizers
  • Melt bondable to a variety of substrates, including PVC
  • Outstanding toughness and puncture resistance
  • Solvent bondable

Product Description: Eastman AP005 is a tough, clear, durable copolyester ether that combines the strength of plastics, the flexibility of elastomers, and the processability of thermoplastics. Eastman AP005 can be used in injection molding and film or tubing extrusion applications or in any application that demands strength, durability, chemical resistance, and puncture resistance in harsh environments. This copolyester combines toughness, clarity, high temperature resistance and flexibility without the addition of plasticizers. Eastman AP005 is considered environmentally preferred because of its non-halogenated material composition. Its broad compatibility with other polymers such as styrenic block copolymers makes it an excellent choice for both alloys and as additives/modifiers to improve performance properties.

Information provided by Eastman.

Vendors:
Available Properties
  • Specific Gravity, ASTM D792
  • Water Absorption, ASTM D570, Immersion
  • Water Vapor Transmission, ASTM F372
  • Oxygen Transmission Rate, ASTM D1434
  • Viscosity Measurement, EMN-A-AC-G-V-1, Inherent
  • Thickness
  • Melt Flow, ASTM D1238
  • Hardness, Shore A, ASTM D2240
  • Hardness, Shore D, ASTM D2240
  • Tensile Strength at Break, ASTM D638
  • Film Tensile Strength at Yield, MD, ASTM D882
  • Film Tensile Strength at Yield, TD, ASTM D882
  • Tensile Strength, Yield, ASTM D638
  • Film Elongation at Break, MD, ASTM D882
  • Film Elongation at Break, TD, ASTM D882
  • Film Elongation at Yield, MD, ASTM D882
  • Film Elongation at Yield, TD, ASTM D882
  • Elongation at Break, ASTM D638
  • Elongation at Yield, ASTM D638
  • Tensile Modulus, ASTM D638
  • Flexural Modulus, ASTM D790
  • Izod Impact, Notched, ASTM D256
  • Coefficient of Friction, ASTM D1894
  • Tear Strength, Total, ASTM D1004
  • Film Tensile Strength at Break, MD, ASTM D882
  • Film Tensile Strength at Break, TD, ASTM D882
  • Tangent Modulus, ASTM D882, T.D.
  • Tangent Modulus, ASTM D882, M.D.
  • Torsional Stiffness, ASTM D1043
  • Torsional Stiffness, ASTM D1043
  • Heat of Fusion, ASTM E793
  • CTE, linear, ASTM D696
  • Specific Heat Capacity, DSC, solid
  • Specific Heat Capacity, DSC, solid
  • Specific Heat Capacity, DSC, solid
  • Specific Heat Capacity, DSC, solid
  • Specific Heat Capacity, DSC, melt
  • Specific Heat Capacity, DSC, transition
  • Thermal Conductivity, ASTM C177
  • Melting Point, ASTM D3418, Crystalline Peak
  • Crystallization Temperature, DSC
  • Vicat Softening Point, ASTM D1525
  • Brittleness Temperature, ASTM D746
  • Glass Transition Temp, Tg, DSC
  • Refractive Index, ASTM D542, nD
  • Haze, ASTM D1003, for Film
  • Gloss, ASTM D2457, for Film, 45°
  • Transmission, Visible, ASTM D1003, Regular, Film
  • Transmission, Visible, ASTM D1003, Total, Film
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Eastman Chemical Company

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.