Notes: Telcar TL-2560A is a general purpose thermoplastic elastomer designed for a variety of industrial applications. Telcar TL-2560A is a low density, medium grade suitable for both injection molding and extrusion. Features: General Purpose; Good Colorability; High Flow; Low Density; Medium Hardness; Low Specific Gravity; Oil Extended Uses: General Purpose; Grommets; Industrial Applications; Industrial Parts Form: Pellets Processing Method: Injection Molding; Extrusion
Injection Notes: Injection Rate: Moderate-Fast Extrusion Notes: Screw Speed: 30 to 100 rpm Information Provided by Teknor Apex |