MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Cookson Group STAYCHIP® 3090.mk.01 High Productivity Capillary Underfill  (discontinued **)
Categories: Polymer; Adhesive; Thermoset

Material Notes: STAYCHIP 3090 is a highly filled, high reliability capillary underfill designed for high productivity flip applications. This material merges excellent stability with fast cure speed, fast flow times, and exceptional reliability performance. The reactivity of Staychip 3090 allows shipment of material in bulk quantities up to 20 ounce cartridges and storage in a conventional refrigerator at 5°C.

Features:

  • 5°C storage
  • Long pot life
  • Non-anhydride formulation
  • Capable to package in large containers to minimize syringe change out
  • Excellent adhesion (even after exposure to high humidity, pressure and temperature)
  • Fast, efficient flow properties
  • High filler loading while maintaining fast flow properties
  • Exceptional reliability in JEDEC testing
  • Proprietary filler technology

Information provided by Cookson Electronics

Vendors:
Available Properties
  • Specific Gravity, ASTM D 1475-60
  • Filler Content
  • Moisture Absorption at Equilibrium, 2 hour boil
  • Particle Size
  • Brookfield Viscosity, Brookfield #51 at 10 RPM
  • Storage Temperature
  • Hardness, Shore D, ASTM D 2240
  • Fracture Toughness
  • CTE, linear, Alpha 1
  • CTE, linear, Alpha 2
  • Glass Transition Temp, Tg, By DSC
  • Flash Point, ASTM D 93-85
  • Pot Life
  • Shelf Life, at 5°C
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.