MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Eastman 7352 PET  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), Unreinforced

Material Notes: VORIDIAN PET thermoplastic polyesters are condensation polymers produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. VORIDIAN PET polyester 7352 is a homopolymer PET that has been crystallized.

Applications/Uses

  • Automotive parts containers
  • Food packaging
  • Household products containers
  • Pharmaceutical containers
  • Medical
  • Health and Nutrition Containers
  • Food-contact containers
  • Vendors:
    Available Properties
    • Specific Gravity, ASTM D792
    • Bulk Density, ASTM D1895, Poured
    • Bulk Density, ASTM D1895, Vibrated
    • Density, ASTM D1505, Crystalline Density
    • Melt Density, ASTM D1238
    • Water Absorption, ASTM D570, 24h Immersion
    • Particle Size, Pellet Size
    • Viscosity Measurement, VGAS-A-AN-G-V-1, Intrinsic
    • Linear Mold Shrinkage, ASTM D955
    • Hardness, Rockwell R, ASTM D785
    • Tensile Strength at Break, ASTM D638
    • Tensile Strength, Yield, ASTM D638
    • Elongation at Yield, ASTM D638
    • Flexural Yield Strength, ASTM D790
    • Flexural Modulus, ASTM D790
    • Izod Impact, Notched, ASTM D256
    • Izod Impact, Notched, ASTM D256
    • Izod Impact, Unnotched, ASTM D4812
    • Izod Impact, Unnotched, ASTM D4812
    • Volume Resistivity, ASTM D257
    • Surface Resistivity per Square, ASTM D257
    • Dielectric Constant, ASTM D150
    • Dielectric Constant, ASTM D150
    • Dielectric Strength, ASTM D149, Short Time, 500V/sec
    • Dissipation Factor, ASTM D150
    • Dissipation Factor, ASTM D150
    • Arc Resistance, ASTM D495
    • Heat of Fusion, ASTM E793
    • Specific Heat Capacity, ASTM E1269
    • Specific Heat Capacity, ASTM E1269
    • Specific Heat Capacity, ASTM E1269
    • Specific Heat Capacity, ASTM E1269
    • Specific Heat Capacity, ASTM E1269
    • Melting Point, ASTM D3418, Crystalline Peak
    • Deflection Temperature at 0.46 MPa (66 psi), ASTM D648
    • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648
    • Vicat Softening Point, ASTM D1525, 1kg load
    • Melt Temperature
    • Mold Temperature
    • Drying Temperature
    • Dry Time
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    Manufacturer Notes:
    Eastman Chemical Company

    Category Notes
    Plastic

    **
    Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

    Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

     

    Rulon Bearings
    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.