Coating Description: SHS 9700 PTAW is an iron based steel alloy with a near nanoscale (submicron) microstructure that features good abrasion and fine particle erosion resistance with no high-cost nickel, tungsten and molybdenum in the material chemistry.Key Performance Characteristics- 67 - 69 HRc single and double pass weld deposits
- Economical iron-based alternative to nickel based materials containing tungsten carbide
- Good resistance to abrasion and erosion from fine particles
- Highly refined microstructure
Application Process: PTAW Weld Overlay for Hardfacing Information Provided by The NanoSteel Company, Inc. |