Available Properties |
---|
- Tensile Strength, Laminate
- Tensile Strength, SACMA SRM-4, 90°, dry
- Tensile Strength, SACMA SRM-4, 90°, dry
- Tensile Strength, SACMA SRM-4, 90°, dry
- Tensile Strength, SACMA SRM-4, 0°, wet
- Tensile Strength, SACMA SRM-4, 0°, dry
- Tensile Strength, SACMA SRM-4, 0°, dry
- Tensile Strength, SACMA SRM-4, 0°, dry
- Tensile Strength, SACMA SRM-4, 0°, dry
- Tensile Modulus, SACMA SRM-4, 90°, dry
- Tensile Modulus, SACMA SRM-4, 90°, dry
- Tensile Modulus, SACMA SRM-4, 90°, dry
- Tensile Modulus, SACMA SRM-4, 0°, dry
- Tensile Modulus, SACMA SRM-4, 0°, dry
- Tensile Modulus, SACMA SRM-4, 0°, dry
- Tensile Modulus, SACMA SRM-4, 0°, dry
- Tensile Modulus, SACMA SRM-4, 0°, wet
- Flexural Strength, 0°, dry, 3-point
- Flexural Strength, 0°, dry, 3-point
- Flexural Modulus, ASTM D790, 0°, dry, 3-point
- Flexural Modulus, ASTM D790, 0°, dry, 3-point
- Compressive Strength, SACMA SRM-1, 0°, wet
- Compressive Strength, SACMA SRM-1, 0°, dry
- Compressive Strength, SACMA SRM-1, 0°, dry
- Compressive Strength, SACMA SRM-1, 0°, dry
- Compressive Strength, SACMA SRM-1, 0°, dry
- Compressive Modulus, SACMA SRM-1, 0°, dry
- Compressive Modulus, SACMA SRM-1, 0°, dry
- Compressive Modulus, SACMA SRM-1, 0°, dry
- Compressive Modulus, SACMA SRM-1, 0°, wet
- Compressive Modulus, SACMA SRM-1, 0°, dry
- Shear Modulus, In-plane, SACMA SRM-7, wet
- Shear Modulus, In-plane, SACMA SRM-7, wet
- Shear Modulus, In-plane, SACMA SRM-7, dry
- Shear Modulus, In-plane, SACMA SRM-7, wet
- Shear Modulus, In-plane, SACMA SRM-7, dry
- Shear Modulus, In-plane, SACMA SRM-7, dry
- Shear Modulus, In-plane, SACMA SRM-7, dry
- Shear Strength, SACMA SRM-8, 0° Short Beam, wet
- Shear Strength, SACMA SRM-8, 0° Short Beam, Water, 160°F (71°C)/14 days
- Shear Strength, SACMA SRM-8, 0° Short Beam, dry
- Shear Strength, SACMA SRM-7, In-plane, wet
- Shear Strength, SACMA SRM-7, In-plane, wet
- Shear Strength, SACMA SRM-8, 0° Short Beam, Fuel, Mil-T-5624, 75°F (24°C)/90 days
- Shear Strength, SACMA SRM-8, 0° Short Beam, Cleaning, Mil-C-87936, 75°F (24°C)/7 days
- Shear Strength, ASTM D740, 0° Short Beam, MEK, 75°F (24°C)/7 days
- Shear Strength, SACMA SRM-8, 0° Short Beam, Hydraulic, Mil-H-83282, 160°F (71°C)/90 days
- Shear Strength, SACMA SRM-8, 0° Short Beam, dry
- Shear Strength, SACMA SRM-8, 0° Short Beam
- Shear Strength, SACMA SRM-8, 0° Short Beam, Deicer, Mil-A-8243, 32°F (0°C)/30 days
- Shear Strength, SACMA SRM-8, 0° Short Beam, Oil, Mil-L-7808, 160°F (71°C)/90 days
- Shear Strength, SACMA SRM-8, 0° Short Beam, Hydraulic, Mil-H-5606, 160°F (71°C)/90 days
- Shear Strength, SACMA SRM-7, In-plane, wet
- Shear Strength, SACMA SRM-8, 0° Short Beam, Oil, Mil-L-23699, 160°F (71°C)/90 days
- Shear Strength, SACMA SRM-7, In-plane, dry
- Shear Strength, SACMA SRM-7, In-plane, dry
- Shear Strength, SACMA SRM-8, 0° Short Beam, dry
- Shear Strength, SACMA SRM-7, In-plane, dry
- Shear Strength, SACMA SRM-7, In-plane, dry
- Maximum Service Temperature, Air
- Gel Time
|
| | |