MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Zell-Metall Engineering Plastics Zellamid 1500 (PEEK)  (discontinued **)
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Unreinforced

Material Notes: Zellamid® 1500 (Polyetheretherketone - PEEK, natural) is the registered trademark for Zell-Metall’s semi-crystalline high performance thermoplastic which exhibits a unique combination of high mechanical properties, temperature resistance and excellent chemical resistance, making it the most popular advanced plastics material.

Fields: Nuclear and Vacuum Technology, Aerospace Industry, Mechanical and Automotive Engineering, Conveyer Technology, Semiconductor Production, Electrical and Electronics, Wire and Cable, Oil Exploration, Chemical Processing Industry.

Besides of the standard grade for tribological applications also our Zellamid® 1500 T grade is available in black color, modified with 10% Carbonfibre, 10% PTFE and 10% Graphite.

Zellamid® 1500 T has an outstanding wear resistance and an even lower coefficient of friction as well as higher Pressure-Velocity capabilities.

Vendors:
Available Properties
  • Density
  • Moisture Absorption at Equilibrium, ISO 1110; DIN 53714, 50% RH
  • Water Absorption at Saturation, ISO 62; DIN 53495, 23°C
  • Tensile Strength at Break, ISO 527; DIN 53455
  • Elongation at Break, ISO 527; DIN 53455
  • Tensile Modulus, ISO 527; DIN 53452
  • Charpy Impact Unnotched, ISO 179; DIN 53453
  • Volume Resistivity, IEC 167; DIN 53482
  • Dielectric Strength, IEC 243; DIN 53481
  • Dissipation Factor, IEC 250; DIN 53483
  • CTE, linear, DIN 53752
  • Thermal Conductivity, DIN 53612 Method A
  • Melting Point, ISO 1218 Method A; DIN 53736
  • Maximum Service Temperature, Air, IEC 216; DIN 53446, 5000 hours; 50% Tensile Strength
  • Maximum Service Temperature, Air, a few hours operation
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75; DIN 53461
  • Flammability, UL94
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.