MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Eastman Tacolyn™ 3570 Resin Dispersion
Categories: Polymer

Material Notes: Product Description: Tacolyn™ 3570 Resin Dispersion is an anionic, aqueous, solvent-free, and APE (alkylphenol ethoxylate) free dispersion of a stabilized rosin ester. It is designed for use in pressure sensitive adhesives based on acrylic polymer emulsions or carboxylated SBR polymer emulsions, where it greatly enhances the tack and peel to polyethylene and carton board.

Application/Uses:

  • Automotive
  • Building and Construction
  • Pressure sensitive adhesives
  • Tapes and Labels
  • Waterborne Adhesives
Key Attributes:
  • APE-free
  • Broad compatibility
  • Excellent silicone liner wetting
  • Excellent thermal and UV stability
  • Good pigment and substrate wetting
  • Good storage and mechanical stability
  • Improves adhesion to polyethylene and polypropylene packaging substrates
  • Light color
  • Low surface tension
  • Outstanding tackifier in waterborne adhesives
  • Resistance to acids and alkalies

Information provided by Eastman

Vendors:
Available Properties
  • Density
  • Solids Content
  • Particle Size
  • pH
  • pH, Tolerance Rang
  • Brookfield Viscosity, RFV at 20 rpm
  • Ring & Ball Softening Point, ASTM E 28
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Eastman Chemical Company

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.