MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
SACO AEI PEXIDAN® HF S/C-UV Moisture Cure XLPE Low Smoke Zero Halogen Jacket
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Description: PEXIDAN® HF S/C-UV is a high performance, low smoke halogen-free, flame retardant, colorable 105°C rated XLPE jacketing system curable by moisture. It consists of a silane pre-grafted base compound SX-0652 and a catalyst masterbatch CM540U/1. Mixed and extruded in the proper proportions (95:5), the two components result in a material that is crosslinkable by exposure to 90°C hot water. Used in conjunction with PEXIDAN® HF X/T UL 44 LSZH insulated conductors, the completed cable would meet LSZH requirements and is FT4 and UL1685-capable. Cables jacketed with PEXIDAN® HF S/C-UV are intended to be marked SUNRES. PEXIDAN® HF S/C-UV is both REACH and RoHS-compliant.

Applications:

  • UL1277 Jacket for Single- and Multi-Conductor Tray-Rated LV and MV Cables
  • Low Smoke Zero Halogen Hazardous Industrial Environments
  • Petrochemical | Transit | Offshore Oil Platforms | Substation Control

Information provided by SACO AEI Polymers.

Vendors:
Available Properties
  • Specific Gravity, ASTM D792
  • Melt Flow, ASTM D1238
  • Melt Flow, ASTM D1238
  • Deformation, UL 1277 / UL 2556
  • Storage Temperature
  • Hardness, Shore A, ASTM D2240
  • Hardness, Shore D, ASTM D2240
  • Tensile Strength at Break, UL 1277 / UL 2556
  • Tensile Strength at Break, UL 1277 / UL 2556, After 60 days oil (OILRES II)
  • Tensile Strength at Break, UL 1277 / UL 2556, Oil (OILRES I)
  • Tensile Strength at Break, UL 1277 / UL 2556, after thermal ageing
  • Tensile Strength at Break, UL 1277 / UL 2556, thermal ageing
  • Elongation at Break, UL 1277 / UL 2556
  • Elongation at Break, UL 1277 / UL 2556, After 60 days oil (OILRES II)
  • Elongation at Break, UL 1277 / UL 2556, Hot, 0.2 N/mm2 load
  • Elongation at Break, UL 1277 / UL 2556, after thermal ageing
  • Elongation at Break, UL 1277 / UL 2556, thermal ageing
  • Elongation at Break, UL 1277 / UL 2556, Oil (OILRES I)
  • Brittleness Temperature, ASTM D638, 3 min in Methanol
  • Smoke Density, ASTM E662, Flaming, corrected
  • Smoke Density, ASTM E662, Non-flaming, corrected
  • Smoke Density, ASTM E662, Flaming
  • Smoke Density, ASTM E662, Non-flaming
  • Oxygen Index, ASTM D2863
  • Processing Temperature, barrel zones
  • Die Temperature
  • Head Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.