MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Pressure Seal 8782 Fluorinated Hydrocarbon
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Compound 8782 is a 75 durometer black colored Viton® GF-S elastomer that is peroxide cured. It exhibits excellent resistance to a wide variety of chemicals including concentrated acids.

This compound will meet or exceed the specifications listed and has the following physical properties: ASTM D2000 2 HK 820 A1-10 B37 B38 EF31 EO78 F15 Z1; 4 HK 820 A1-11 B38 EF31 EO78 Z1; 6 HK 820 A1-10 A1-11 B31 B38 EO88 F15 Z1
Z1 = 75 ± 5 Shore A Durometer

Information provided by Pressure Seals Inc.

Vendors:
Available Properties
  • Specific Gravity
  • Hardness, Shore A
  • Hardness, Shore A, Concentrated Nitric Acid
  • Hardness, Shore A, 50% MeOH/50% FUEL C
  • Hardness, Shore A, 50% MeOH/50% FUEL C
  • Hardness, Shore A, 50% MeOH/50% FUEL C
  • Hardness, Shore A, 15% EtOH/85% FUEL C
  • Hardness, Shore A, 50% MeOH/50% FUEL C
  • Hardness, Shore A, 15% EtOH/85% FUEL C
  • Hardness, Shore A, Stauffer Blend 7700
  • Hardness, Shore A, 15% EtOH/85% FUEL C
  • Hardness, Shore A, Methanol
  • Hardness, Shore A, 85% EtOH/15% FUEL C
  • Hardness, Shore A, Methanol
  • Hardness, Shore A, Methanol
  • Hardness, Shore A, 85% EtOH/15% FUEL C
  • Hardness, Shore A, 85% EtOH/15% FUEL C
  • Hardness, Shore A, Service Fluid 101
  • Hardness, Shore A, Ethanol
  • Hardness, Shore A, Methanol
  • Hardness, Shore A, 15% EtOH/85% FUEL C
  • Hardness, Shore A, Concentrated Nitric Acid
  • Hardness, Shore A, ASTM Oil #1 (IRM 901)
  • Hardness, Shore A, Sodium Hypochlorite
  • Hardness, Shore A, Ethanol
  • Hardness, Shore A, 85% EtOH/15% FUEL C
  • Hardness, Shore A, Hydrochloric Acid 37%
  • Hardness, Shore A, Hydrochloric Acid 37%
  • Hardness, Shore A, Ethanol
  • Hardness, Shore A, ASTM Oil #3 (IRM 903)
  • Hardness, Shore A, Ethanol
  • Hardness, Shore A, Sodium Hydroxide (50%)
  • Hardness, Shore A, Sodium Hydroxide (50%)
  • Hardness, Shore A, Hydrochloric Acid 37%
  • Hardness, Shore A, Concentrated Nitric Acid
  • Hardness, Shore A, Sodium Hypochlorite
  • Hardness, Shore A, ASTM Reference Fuel C
  • Hardness, Shore A, Concentrated Sulfuric Acid
  • Hardness, Shore A, Concentrated Sulfuric Acid
  • Hardness, Shore A, Concentrated Sulfuric Acid
  • Hardness, Shore A, Sodium Hypochlorite
  • Hardness, Shore A, Heat Aged
  • Hardness, Shore A, Heat Aged
  • Hardness, Shore A, ASTM Reference Fuel A
  • Hardness, Shore A, Sodium Hydroxide (50%)
  • Tensile Strength
  • Tensile Strength, Hydrochloric Acid 37%
  • Tensile Strength, Concentrated Sulfuric Acid
  • Tensile Strength, ASTM Reference Fuel A
  • Tensile Strength, ASTM Reference Fuel C
  • Tensile Strength, Stauffer Blend 7700
  • Tensile Strength, Service Fluid 101
  • Tensile Strength, Concentrated Sulfuric Acid
  • Tensile Strength, Sodium Hypochlorite
  • Tensile Strength, ASTM Oil #3 (IRM 903)
  • Tensile Strength, Concentrated Nitric Acid
  • Tensile Strength, ASTM Oil #1 (IRM 901)
  • Tensile Strength, Sodium Hydroxide (50%)
  • Tensile Strength, Heat Aged
  • Tensile Strength, Heat Aged
  • Elongation, Ultimate
  • Elongation, Ultimate, ASTM Reference Fuel A
  • Elongation, Ultimate, Sodium Hypochlorite
  • Elongation, Ultimate, ASTM Oil #1 (IRM 901)
  • Elongation, Ultimate, ASTM Reference Fuel C
  • Elongation, Ultimate, Hydrochloric Acid 37%
  • Elongation, Ultimate, ASTM Oil #3 (IRM 903)
  • Elongation, Ultimate, Sodium Hydroxide (50%)
  • Elongation, Ultimate, Stauffer Blend 7700
  • Elongation, Ultimate, Concentrated Nitric Acid
  • Elongation, Ultimate, Concentrated Sulfuric Acid
  • Elongation, Ultimate, Service Fluid 101
  • Elongation, Ultimate, Concentrated Sulfuric Acid
  • Elongation, Ultimate, Heat Aged
  • Elongation, Ultimate, Heat Aged
  • 100% Modulus
  • Tear Strength, Die B
  • Tear Strength, Die C
  • Compression Set, Plied
  • Compression Set, Plied
  • Compression Set, Plied
  • Brittleness Temperature
  • Shrinkage, Volume, Sodium Hydroxide (50%)
  • Shrinkage, Volume, Sodium Hydroxide (50%)
  • Shrinkage, Volume, Sodium Hydroxide (50%)
  • Shrinkage, Volume, Sodium Hypochlorite
  • Shrinkage, Volume, Sodium Hypochlorite
  • Shrinkage, Volume, Sodium Hypochlorite
  • Shrinkage, Volume, ASTM Reference Fuel A
  • Shrinkage, Volume, ASTM Oil #1
  • Shrinkage, Volume, Ethanol
  • Shrinkage, Volume, Ethanol
  • Shrinkage, Volume, 85% EtOH/15% FUEL C
  • Shrinkage, Volume, ASTM Reference Fuel C
  • Shrinkage, Volume, ASTM Oil #3
  • Shrinkage, Volume, Methanol
  • Shrinkage, Volume, 85% EtOH/15% FUEL C
  • Shrinkage, Volume, Ethanol
  • Shrinkage, Volume, Hydrochloric Acid 37%
  • Shrinkage, Volume, 15% EtOH/85% FUEL C
  • Shrinkage, Volume, Hydrochloric Acid 37%
  • Shrinkage, Volume, Concentrated Nitric Acid
  • Shrinkage, Volume, Ethanol
  • Shrinkage, Volume, Methanol
  • Shrinkage, Volume, 85% EtOH/15% FUEL C
  • Shrinkage, Volume, Concentrated Sulfuric Acid
  • Shrinkage, Volume, Concentrated Sulfuric Acid
  • Shrinkage, Volume, 15% EtOH/85% FUEL C
  • Shrinkage, Volume, Concentrated Nitric Acid
  • Shrinkage, Volume, 50% MeOH/50% FUEL C
  • Shrinkage, Volume, Service Fluid 100
  • Shrinkage, Volume, Methanol
  • Shrinkage, Volume, 85% EtOH/15% FUEL C
  • Shrinkage, Volume, Methanol
  • Shrinkage, Volume, Stauffer Blend 7700
  • Shrinkage, Volume, 50% MeOH/50% FUEL C
  • Shrinkage, Volume, Concentrated Sulfuric Acid
  • Shrinkage, Volume, 15% EtOH/85% FUEL C
  • Shrinkage, Volume, Hydrochloric Acid 37%
  • Shrinkage, Volume, 15% EtOH/85% FUEL C
  • Shrinkage, Volume, 50% MeOH/50% FUEL C
  • Shrinkage, Volume, 50% MeOH/50% FUEL C
  • Shrinkage, Volume, Concentrated Nitric Acid
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.