MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
HB Fuller 2536 Silicone system
Categories: Polymer; Thermoset; Silicone

Material Notes: 2536 is two-component, room temperature fast Bonding silicone system. Typical applications include glass, metal and plastic bonding. It has very good long term adhesion performance in high temperature conditions. 2536 is black RTV-2 silicone, which is fast curing and with good adhesion to a variety of materials. 2536 is a de-alcoholized silicone with the advantages of low odor, no solvent, no corrosion, and it also has excellent electric performance and excellent resistance to all kinds of weather such as UV light, rainwater and hailstone impacting, etc. There is a secondary cure with atmospheric moisture that promotes full cure over 7 days.

Features and Benefits:

  • Fast curing
  • RoHS compliant and Halogen free
  • Non-corrosive, low odor
  • Excellent adhesion to a wide variety of substrates including glass, metal and plastics
  • Wide operating temperature range
  • Very fast setting and fast curing enabling reduced production times/ul>Typical Applications:
    • Seam sealing• Bonding to Glass, Plastic and Metals
    • Bonding and sealing in appliance applications
    • General assembly sealing

    Information provided by H.B. Fuller Company

Vendors:
Available Properties
  • Specific Gravity
  • Storage Temperature
  • Hardness, Shore A, GB/T531
  • Hardness, Shore A, GB/T531, Damp Heat Aging Testing; 85% RH
  • Tensile Strength, GB/528
  • Tensile Strength, GB/528, Damp Heat Aging Testing; 85% RH
  • Elongation at Break, GB/528
  • Elongation at Break, GB/528, Damp Heat Aging Testing; 85% RH
  • Shear Strength, GB/T7124, Lap Joint, Aluminum
  • Shear Strength, GB/T7124, Damp Heat Aging Testing; 85% RH
  • Volume Resistivity, GB/T1692
  • Dielectric Strength, GB/T1695
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Cure Time, Working Time
  • Cure Time, Fixture Time
  • Cure Time, 7 days at (50±5)%RH
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.