MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Resinlab® UR3010 Clear Polyurethane Potting System
Categories: Polymer; Adhesive; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Adhesive

Material Notes: Resinlab™ UR 3010 Clear is a, two component, room temperature curing polyurethane potting system. It is designed to cure completely at room temperature. UR 3010 provides excellent environmental protection giving very good resistance to water, salt spray, inorganic acids and bases, and most organic solvents, while maintaining tenacious adhesion to various metals, plastics and other common assembly materials. UR 3010 Clear is an unfilled system that has a high degree of flexibility at temperatures as low as –40C. It provides excellent moisture resistance and can withstand 125°C continuous operation. Excursions to 150C for < 24 hours have no detectable effect on hardness or produces measureable weight loss. It also has a low viscosity, which facilitates flow and penetration into difficult areas. This product was formulated to a convenient mixing ratio of 1 to 1 by volume. It is well suited to automated meter mix operations. UR 3010 Clear is a DOT non-hazardous material and contains no TDI, MOCA, or other reportable substances. Part B is moisture sensitive and must be kept away from atmospheric moisture during storage. After opening a sealed container, thoroughly purge the remaining air space with dry nitrogen (or equivalent) before closing the container.

Information Provided by Resinlab L.L.C., an Ellsworth Adhesives Company.

Vendors:
Available Properties
  • Specific Gravity, Part A
  • Specific Gravity, Mixed
  • Specific Gravity, Part B
  • Viscosity, Part B
  • Viscosity, Mixed
  • Viscosity, Part A
  • Hardness, Shore A
  • Tensile Strength, Yield
  • Tensile Strength, Yield, at 100%
  • Elongation at Break
  • Volume Resistivity
  • Dielectric Constant
  • Dielectric Strength
  • CTE, linear
  • Maximum Service Temperature, Air
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Transmission, Visible, clear; thickness not quantified
  • Cure Time
  • Cure Time
  • Pot Life, Mass: 100g
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.