MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Hexcel® HexFlow® RTM230ST Mono-component Epoxy System
Categories: Polymer; Thermoset; Epoxy

Material Notes: Description: HexFlow® RTM230ST is an aerospace qualified mono-component resin system specially developed for Liquid Composite Molding applications, particularly RTM processes. HexFlow® RTM230ST is ideal for engines applications, such as fan blades, containment cases and OGVs due to its high toughness & Tg long term thermal stability. HexFlow® RTM230ST can be used in combination with a wide range of HexForce®, 2,5D & 3D fabrics. If needed, binders and veils are also available and fully compatible with HexFlow® RTM230ST. They provide easy preforming properties, reinforcement dimensional stability and toughening properties.

Advantages

  • Qualified for RTM process
  • Low moisture absorption: < 1,5%
  • High toughness & high-rate impact resistance
  • Glass transition temperatures: dry1: Tg>160°C; wet2: Tg>140°C
  • Tg long-term thermal stability

Information provided by Hexcel Corporation.

Vendors:
Available Properties
  • Density
  • Moisture Absorption
  • Viscosity, 3°C/min
  • Viscosity, 2°C/min
  • Viscosity, 1°C/min
  • Viscosity, 0.5°C/min
  • Viscosity, 1°C/min
  • Viscosity, 2°C/min
  • Viscosity, 3°C/min
  • Viscosity, 0.5°C/min
  • Viscosity, 0.5°C/min
  • Viscosity, 1°C/min
  • Viscosity, 2°C/min
  • Viscosity, 3°C/min
  • Tensile Strength, Ultimate, ASTM D638, Wet
  • Tensile Strength, Ultimate, ASTM D638, Dry
  • Tensile Strength, Ultimate, ASTM D638, Wet
  • Tensile Strength, Ultimate, ASTM D638, Dry
  • Tensile Modulus, ASTM D638, Wet
  • Tensile Modulus, ASTM D638, Dry
  • Tensile Modulus, ASTM D638, Wet
  • Tensile Modulus, ASTM D638, Dry
  • Compressive Yield Strength, ASTM D695, Wet
  • Compressive Yield Strength, ASTM D695, Dry
  • Compressive Yield Strength, ASTM D695, Wet
  • Compressive Yield Strength, ASTM D695, Dry
  • Compressive Strength, ASTM D7136/ D7137, after 30J impact
  • Compressive Strength, ASTM D695, Ultimate, Dry
  • Compressive Strength, ASTM D695, Ultimate, Wet
  • Compressive Strength, ASTM D695, Ultimate, Dry
  • Compressive Strength, ASTM D695, Ultimate, Wet
  • Compressive Strength, EN2850A1, 90°, Ultimate, Wet
  • Compressive Strength, EN2850A1, 0°, Ultimate, Wet
  • Compressive Strength, EN2850A1, 90°, Ultimate, Dry
  • Compressive Strength, EN2850A1, 0°, Ultimate, Dry
  • Compressive Strength, EN2850A1, 90°, Ultimate, Wet
  • Compressive Strength, EN2850A1, 0°, Ultimate, Wet
  • Compressive Strength, EN2850A1, 90°, Ultimate, Dry
  • Compressive Strength, EN2850A1, 0°, Ultimate, Dry
  • Compressive Modulus, ASTM D695, Wet
  • Compressive Modulus, ASTM D695, Dry
  • Compressive Modulus, ASTM D695, Dry
  • Compressive Modulus, ASTM D695, Wet
  • Compressive Modulus, EN2850A1, 0°, Wet
  • Compressive Modulus, EN2850A1, 90°, Dry
  • Compressive Modulus, EN2850A1, 0°, Dry
  • Compressive Modulus, EN2850A1, 90°, Dry
  • Compressive Modulus, EN2850A1, 90°, Wet
  • Compressive Modulus, EN2850A1, 0°, Wet
  • Compressive Modulus, EN2850A1, 0°, Dry
  • Compressive Modulus, EN2850A1, 90°, Wet
  • Fracture Toughness
  • Shear Modulus, EN6031, In plane, Dry
  • Shear Modulus, EN6031, In plane, Wet
  • Shear Modulus, EN6031, In plane, Dry
  • Shear Modulus, EN6031, In plane, Wet
  • Shear Strength, EN6031, Ultimate, In plane, Wet
  • Shear Strength, EN6031, Ultimate, In plane, Dry
  • Shear Strength, EN6031, Ultimate, In plane, Wet
  • Shear Strength, EN6031, Ultimate, In plane, Dry
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • Glass Transition Temp, Tg, midpoint
  • Glass Transition Temp, Tg, onset endo
  • Glass Transition Temp, Tg, peak endo
  • Glass Transition Temp, Tg, onset
  • Glass Transition Temp, Tg, peak
  • Gel Time, Time to reach 200 mPa.s
  • Gel Time, Time to reach 200 mPa.s
  • Gel Time, Time to reach 1000 mPa.s
  • Gel Time, Time to reach 1000 mPa.s
  • Gel Time, Time to reach 200 mPa.s
  • Gel Time, Time to reach 200 mPa.s
  • Gel Time, G’ & G’’ crossover
  • Gel Time, Time to reach 1000 mPa.s
  • Gel Time, Time to reach 200 mPa.s
  • Gel Time, Time to reach 1000 mPa.s
  • Gel Time, G’ & G’’ crossover
  • Gel Time, Time to reach 1000 mPa.s
  • Gel Time, G’ & G’’ crossover
  • Gel Time, Time to reach 1000 mPa.s
  • Gel Time, G’ & G’’ crossover
  • Gel Time, Time to reach 1000 mPa.s
  • Gel Time, G’ & G’’ crossover
  • Gel Time, Time to reach 1000 mPa.s
  • Gel Time, G’ & G’’ crossover
  • Gel Time, G’ & G’’ crossover
  • Gel Time, G’ & G’’ crossover
  • Gel Time, G’ & G’’ crossover
  • Gel Time, G’ & G’’ crossover
  • Gel Time, G’ & G’’ crossover
  • Shelf Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.