Description: Kraton G1650 E is a clear linear triblock copolymer based on styrene and ethylene/butylene, S-E/B-S, with bound styrene of 29.2% mass. It is supplied from Europe in the physical forms identified: Kraton G1650 EU - supplied as undusted fluffy crumb Kraton G1650 ES - supplied as fluffy crumb dusted with amorphous silicaRegion: Asia Pacific, Europe, Japan, North America, and South America Uses: Kraton G1650 E is used for formulating adhesives and coatings, as a base material for compound formulations, as a modifier of thermoplastics and as a modifier of bitumen. The inherent stability of the midblock suggests the use of G1650 E in applications that must withstand weathering and high processing temperatures. Applications: Adhesives, Sealant and Coatings; Compounding and Personal Hygiene; Impact Modification; Medical; Packaging and Polymod; Personal Care; Bitumen Modification; and Roads and Roofing |