NanoActive MgO is produced using proprietary processes to obtain high specific surface area, small crystallite size material possessing high chemical reactivity, particularly at elevated temperatures. Applications: Applications include destruction of chemical warfare agents, destructive adsorption of acid gases and polar organic molecules, fertilizers, nanocomposites, phosphor particle protection layer, precursor for other magnesium chemicals, remediation of toxic waste, sintering aid, and waste water treatment. Information provided by NanoScale Composition based on metal |