MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Henkel Loctite® Stycast® 2762 with CAT 14 Epoxy
Categories: Polymer; Thermoset; Epoxy; Epoxy Encapsulant, Unreinforced

Material Notes: Loctite Stycast 2762 provides the following product characteristics:
  • High temperature resistance
  • Low coefficient of thermal expansion
  • Low shrinkage during cure
  • Excellent adhesion to metals, glass or plastic materials

Cure: Heat cure

Application: Potting, Encapsulation

Loctite Stycast 2762 is used to embed electronic compounds to hermetically sealed metal surfaces. It is also designed to act as a high temperature resistant protective coating.

Loctite Stycast 2762 can be used with a variety of catalysts.

CATALYST DESCRIPTION

Loctite CAT 14 provides the following product characteristics:

  • Powdered epoxy hardener
  • Use for powdered for paste applications
  • Chemical resistant
  • High temperature performance
  • Long work life

Cure: Heat cure

Information provided by Henkel.

Vendors:
Available Properties
  • Density, Part A, Loctite Stycast 2762
  • Viscosity, Part A, Loctite Stycast 2762
  • Cure Time, For improved high temperature properties, cure for an additional 3 hours @ 150°C.
  • Shelf Life, Part A, Loctite Stycast 2762
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Loctite Division of Henkel

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.