MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Northstar Polymers MPP-A60A Liquid Castable Polyurethane
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Liquid

Material Notes: MPP-A60A is a room-temperature-cure liquid castable polyurethane system. This ether-base polyurethane system is used in applications such as mold-making, prototyping, production of cast parts, potting, tool-making, and many other applications. MPP-A60A is designed for an easy operation for industrial applications without special casting or heating equipment. Its low viscosity also makes it easy to achieve replicating the details of the mold/original with a fine resolution. Urethane elastomer parts made of this system exhibit:
  • Fine resolution of mold details
  • Good cut/tear resistance for its class
  • Good performance in wet environments
  • Easy-to-use room-temperature-curable
  • Small shrinkage factor

The suitable applications of MPP-A60A include stamps/patterns and molds designed to transfer a decorative image to wet surfaces as well as a potting compound for electronic applications where low viscosity liquid resin is required to encapsulate small wires and components. It is also suitable for many other custom applications where flexibility and strength of the parts are required.

Information provided by Northstar Polymers.

Vendors:
Available Properties
  • Hardness, Shore A, ASTM D2240
  • Tensile Strength, ASTM D412
  • Elongation at Break, ASTM D412
  • Rebound, ASTM D2632, Bashore Rebound
  • Tear Strength, ASTM D624, Split
  • Tear Strength, ASTM D624, Die C
  • Processing Temperature, Prepolymer Temperature
  • Processing Temperature, Curing Agent Temperature
  • Mold Temperature
  • Cure Time, De-mold Time
  • Cure Time, Complete Cure Cycle
  • Pot Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.