MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Raschig Group 3592 Epoxy  (discontinued **)
Categories: Polymer; Thermoset; Epoxy; Epoxy, Molded, Glass Fiber Filler; Filled/Reinforced Thermoset

Material Notes: Glass fiber-reinforced and inorganically filled epoxy molding compound (EP) in color black. Good mechanical strength, long term retention of electrical properties, high tracking resistance (CTI 600) and good dimensional stability also at high temperatures. Self-extinguishing (V-0/0.8 according to UL 94). Free of halogens and toxic heavy metals. Form: Low dust granulate packed in moisture resistant cartons, Standard carton size: 25 kg palletized in 750 kg loads. Processing: Compression/Transfer/Injection.

Information provided by the Raschig Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.95 - 2.05 g/ccISO 1183
Apparent Bulk Density 0.800 - 0.900 g/ccISO 60
Linear Mold Shrinkage 0.0015 - 0.0025 cm/cmInjection; ISO 2577
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 50.0 - 60.0 MPaInjection; ISO 527
Elongation at Break 1.0 - 1.2 %Injection; ISO 527
Modulus of Elasticity 6.00 - 8.00 GPaInjection; ISO 527
Flexural Strength 130 - 150 MPaInjection; ISO 178
Flexural Modulus 13.0 - 16.0 GPaInjection; ISO 178
Compressive Strength 120 - 140 MPaInjection; ISO 604
Charpy Impact Unnotched 1.20 - 1.60 J/cm²
@Temperature 23.0 °C
Injection; ISO 179/ 1eU
Charpy Impact, Notched 0.600 - 0.700 J/cm²
@Temperature 23.0 °C
Injection; ISO 179/ 1eA
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index >= 600 VCTI-M; IEC 60112
 >= 600 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) >= 200 °CInjection; ISO 75-B
Deflection Temperature at 1.8 MPa (264 psi) >= 200 °CInjection; ISO 75-A
Deflection Temperature at 8.0 MPa >= 160 °CInjection; ISO 75-C
Flammability, UL94 V-0
@Thickness 0.800 mm
Shrinkage 0.00 - 0.050 %Post-shrinkage; ISO 2577
 
Processing PropertiesOriginal ValueComments
Front Barrel Temperature 50.0 - 70.0 °C
Melt Temperature 90.0 - 100 °C
Mold Temperature 160 - 180 °C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Raschig Group EPOXIDUR® 3580 EP Epoxy
Cosmic Plastics E484 Glass Filled Epoxy Molding Compound, Electrical Grade
Cookson Group Plaskon® 435 Mineral Filled Epoxy Molding Compound
Sumitomo Bakelite North America Epiall® 2061B-1 Mineral and Glass Filled Electrical Encapsulation Grade Epoxy
Sumitomo Bakelite North America Epiall® 1908-1 Short Glass Fiber Reinforced Epoxy

PRASCH00 / 65285

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.