MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Biomerics Quadraflex™ ARE 80A- B20 Aromatic Polyether TPU
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Quadraflex™ ARE is a family of aromatic polyether-based medical grade thermoplastic urethanes. Quadraflex ARE exhibits excellent mechanical properties, biocompatibility, and toughness. Quadraflex ARE is the most common medical grade urethane family and is used across a range of medical markets including venous access, urology, hemodialysis, respiratory, fluid management, balloons, and minimally invasive surgical devices. It is USP Class VI and ISO-10993 compliant.

Characteristics: Excellent mechanical properties, good chemical resistance, elasticity, biocompatibility, toughness, hemocompatable.

Applications: Extrusion, Injection Molding, Solution

Information provided by Biomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.29 g/ccASTM D792
Linear Mold Shrinkage 0.0080 - 0.012 in/inASTM 955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 80ASTM D2240
Tensile Strength, Ultimate 4200 psiASTM D412
Elongation, Ultimate 650 %ASTM D412
100% Modulus 750 psi
@Strain 100 %
ASTM D412
300% Modulus 1200 psi
@Strain 300 %
ASTM D412
Flexural Modulus 1800 psiASTM D790
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 171 °CInjection
Front Barrel Temperature 185 °CInjection
Nozzle Temperature 191 °CInjection
Zone 1 149 °CExtrusion
Zone 2 160 °CExtrusion
Zone 3 171 °CExtrusion
Zone 4 177 °CExtrusion
Adapter Temperature 177 °CExtrusion
Die Temperature 188 - 210 °CExtrusion
Melt Temperature 191 °CInjection
Mold Temperature 10.0 - 27.0 °CInjection
Drying Temperature 60.0 °C
@Time >=14400 sec
Dew Point -40.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBIOMC070 / 250946

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.