Moplen RP340H is a clarified random copolymer for extrusion applications. The grade exhibits high transparency and medium stiffness. Moplen RP340H is typically used in co-extrusion blow molding, sheet extrusion and thermoforming applications. Applications: Bottles For Consumer Goods, Bottles for Industrial Use.Information provided by LyondellBasell. |