MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Möller Medical NanoSkin 94 NanoCoating
Categories: Ceramic; Glass; Glass Ceramic; Other Engineering Material; Ceramic/Metallic Coating

Material Notes: Non-abrasive coating with extreme chemical resistance, easy-to-clean, biocompatible, also for plastics.

Information provided by Möller Medical, Member of CENTROTEC Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 5.00 - 5.00 microns
 
Mechanical PropertiesOriginal ValueComments
Taber Abrasion, mg/1000 Cycles 11CS17 friction disc with 500g load; DIN 53754
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 200 °C
 
Processing PropertiesOriginal ValueComments
Processing Temperature 80.0 - 150 °CHardening Temperature
 
Descriptive Properties
Applicable SubstrateABSwith restrictions
 Aluminum
 Brass
 Copper
 Glass
 Nylon
 PMMA
 Polycarbonate
 Stainless Steel
 Tubes int. dia. 0.1-10 mm
BiocompatibilityBiocompatibleOne-parametric cytotoxicity test
Contact Angle to Water [deg]94
Cupping Test [mm]1.5DIN EN ISO 1520
Pendulum Dampening Test [sec]140-160DIN EN ISO 1522

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Ateva® 1081G Medical Grade EVA
AdvanSource Biomaterials ChronoFlex® AL 55D Biodurable Medical Grade Polyurethane
Accuratus MACOR Machinable Glass Ceramic
712-6 Nextrema® Translucent Blue-Grey Glass Ceramic/SCHOTT
ELASTO UK Mediprene™ 500900M TPE, Medical Applications, 90A Hardness

CMOLL05 / 1626

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.