MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Owens Corning Glass Fiber Reinforced Polyphenylene Sulfide, 40 wt.% glass
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler

Material Notes: Polyphenylene Sulfide provides excellent resistance to organic solvents (below 375°F). It is unaffected by strong alkalis or aqueous organic salt solutions. Data provided by the manufacturer, Owens Corning.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.64 g/ccASTM D792
Water Absorption 0.010 %24 hrs.; ASTM D570
Linear Mold Shrinkage 0.0020 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 123ASTM D785
Tensile Strength, Ultimate 150 MPaASTM D638
Elongation at Break 3.0 %ASTM D638
Modulus of Elasticity 14.1 GPaASTM D638
Flexural Strength 260 MPaASTM D790
Flexural Modulus 13.0 GPaASTM D790
Compressive Strength 140 MPaASTM D695
Izod Impact, Notched 0.800 J/cm
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 4.00e+15 ohm-cmASTM D257
Dielectric Constant 3.0
@Frequency 60 Hz
ASTM D150
Dielectric Strength 380 V/milASTM D149
Arc Resistance 125 secASTM D495
 
Thermal PropertiesOriginal ValueComments
Flammability, UL94 V-0V-O/5V

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Omnia Plastica PPS GF40 Polyphenylenesulphide
LG Chemical LUSEP GP2400 PPS+GF40%, General Purpose
Oxford Polymers PPS-40GF PPS, 40% Glass Fiber Reinforced
Toyobo TS401 PPS, 40% Glass Fiber Reinforced
Oxford Polymers 40GF 40% Glass Fiber Reinforced Polyphenylene Sulfide

POC017 / 55595

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.