MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Overview of materials for Acrylic, Optical Grade, Molded
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, Optical Grade, Molded

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Optical Grade, Molded". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.11 - 1.19 g/ccAverage value: 1.18 g/cc Grade Count:131
Water Absorption 0.300 %Average value: 0.300 % Grade Count:24
Water Absorption at Saturation 0.300 - 2.00 %Average value: 0.867 % Grade Count:3
Particle Size 230 - 600 µmAverage value: 538 µm Grade Count:6
Viscosity 2.00e+6 - 2.00e+6 cP
@Temperature 240 - 240 °C
Average value: 2.00e+6 cP Grade Count:1
 2.00e+6 - 2.00e+6 cP
@Shear Rate 100 - 100 1/s
Average value: 2.00e+6 cP Grade Count:1
Linear Mold Shrinkage 0.00200 - 0.00800 cm/cmAverage value: 0.00420 cm/cm Grade Count:128
Melt Flow 0.700 - 40.0 g/10 minAverage value: 10.5 g/10 min Grade Count:131
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 48.0 - 99.0Average value: 85.6 Grade Count:31
Tensile Strength, Ultimate 38.0 - 89.3 MPaAverage value: 59.7 MPa Grade Count:124
Tensile Strength, Yield 54.0 - 72.0 MPaAverage value: 67.5 MPa Grade Count:8
Elongation at Break 2.00 - 40.0 %Average value: 8.79 % Grade Count:125
Elongation at Yield 2.00 - 6.00 %Average value: 3.65 % Grade Count:10
Modulus of Elasticity 1.76 - 3.65 GPaAverage value: 2.87 GPa Grade Count:122
Flexural Yield Strength 48.3 - 124 MPaAverage value: 95.0 MPa Grade Count:131
Flexural Modulus 2.00 - 82.0 GPaAverage value: 6.73 GPa Grade Count:21
Izod Impact, Notched 0.160 - 1.30 J/cmAverage value: 0.302 J/cm Grade Count:124
 0.26695 - 0.800 J/cm
@Temperature 0.000 - 0.000 °C
Average value: 0.516 J/cm Grade Count:3
 0.26695 - 0.800 J/cm
@Diameter 6.35 - 6.35 mm
Average value: 0.516 J/cm Grade Count:3
Izod Impact, Notched (ISO) 1.70 - 2.20 kJ/m²Average value: 1.85 kJ/m² Grade Count:6
Charpy Impact Unnotched 1.80 - 2.60 J/cm²Average value: 2.00 J/cm² Grade Count:6
Charpy Impact, Notched 0.200 - 1.80 J/cm²Average value: 0.592 J/cm² Grade Count:9
Gardner Impact 0.226 - 9.04 JAverage value: 1.55 J Grade Count:104
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 3.40 - 3.80Average value: 3.67 Grade Count:8
Dielectric Strength 18.0 - 45.0 kV/mmAverage value: 21.4 kV/mm Grade Count:8
Dissipation Factor 0.0400 - 0.0500Average value: 0.0471 Grade Count:7
 
Thermal PropertiesOriginal ValueComments
CTE, linear 30.0 - 120 µm/m-°CAverage value: 68.4 µm/m-°C Grade Count:125
 72.0 - 72.0 µm/m-°C
@Temperature 0.000 - 156 °C
Average value: 72.0 µm/m-°C Grade Count:2
Specific Heat Capacity 1.30 - 1.50 J/g-°CAverage value: 1.44 J/g-°C Grade Count:11
 1.90 - 2.30 J/g-°C
@Temperature 100 - 175 °C
Average value: 2.10 J/g-°C Grade Count:3
Thermal Conductivity 0.190 - 0.220 W/m-KAverage value: 0.205 W/m-K Grade Count:11
Melting Point 132 - 157 °CAverage value: 150 °C Grade Count:7
Maximum Service Temperature, Air 50.0 - 100 °CAverage value: 78.1 °C Grade Count:61
Deflection Temperature at 0.46 MPa (66 psi) 91.0 - 106 °CAverage value: 100 °C Grade Count:7
Deflection Temperature at 1.8 MPa (264 psi) 60.0 - 104 °CAverage value: 85.4 °C Grade Count:131
Vicat Softening Point 75.6 - 117 °CAverage value: 102 °C Grade Count:122
Flammability, UL94 HBGrade Count:80
Glow Wire Test 650 °CAverage value: 650 °C Grade Count:6
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.49 - 1.51Average value: 1.49 Grade Count:22
Haze 0.400 - 12.0 %Average value: 1.40 % Grade Count:120
Yellow Index -0.400 - 1.00 %Average value: 0.750 % Grade Count:8
Transmission, Visible 84.0 - 92.0 %Average value: 91.6 % Grade Count:130
UV Transmittance 49.5 - 92.0 %Average value: 77.6 % Grade Count:5
 
Processing PropertiesOriginal ValueComments
Melt Temperature 193 - 260 °CAverage value: 233 °C Grade Count:8
Mold Temperature 26.7 - 79.4 °CAverage value: 55.0 °C Grade Count:7
Drying Temperature 71.1 - 79.4 °CAverage value: 77.5 °C Grade Count:7

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Acrylic, General Purpose, Molded
Overview of materials for Acrylic, Optical Sheet
Overview of materials for Acrylic, Cast
Overview of materials for Acrylic, Extruded
Overview of materials for Acrylic, Heat Resistant, Molded

O1306 / 77865

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.