MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Arya Sasol HBM 5510 High Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Product Description: HBM5510 is a high density polyethylene, specially developed for large blow molding parts. This grade offer high stiffness, good processability and good ESCR. HBM5510 has been manufactured under Basell license.

Application: Large blow molding parts, standard and lightweight Jerry cans

Forms: Pellets

Attribute: Good ESCR, good stiffness, good processability

Additives: Antioxidant: Yes; Processing Aid: No; Antiblock: No; Slip Agent: No

Information provided by

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density >= 0.500 g/ccISO 60
Density 0.955 g/ccISO 1183
Environmental Stress Crack Resistance 90 hourBasell method
Melt Flow 10 g/10 min
@Load 21.6 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 49.0 MPaISO 2039-1
Tensile Strength, Yield 27.0 MPaISO 527-1, -2
Elongation at Yield 8.0 %ISO 527-1, -2
Modulus of Elasticity 1.10 GPaISO 527-1, -2
Tensile Impact Strength 135 kJ/m²
@Temperature -30.0 °C
Notched, Type 1, Method 1B; ISO 8256/1B
 
Processing PropertiesOriginal ValueComments
Processing Temperature 180 - 220 °CExtruder temperature profile
Melt Temperature 200 - 235 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PARYA012 / 250466

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.