ABS730Z is heat resistance ABS with low gloss, high rigidity, toughness and good UV stability. Application: Hair dryer shells, electric oven exterior parts and microwave ovens etc Features: High rigidity; High toughness Information provided by Shanghai Kumho Sunny Plastics co, Ltd |