Diaflora® is an elastic monofilament and fabric. The monofilament has optimum rigidity and superior elongation recovery, thick glossy finish available in shades ranging from milky white to black, no yielding point with excellent linear elasticity, and does not emit any toxic gases such as hydrogen cyanide when subject to heat. Grade DS 2220B contains no thermal bonding content. |