MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) KetaSpire® MS NT1 AM Filament PEEK
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK)

Material Notes: Ketaspire® MS NT1 AM Filament provides long-term performance up to 240 °C, including exceptional chemical resistance, outstanding wear and abrasion resistance. These properties make it particularly suited for metal replacement in critical applications in severe end-use environments, such as Oil & Gas, Aerospace and Automotive.

Applications: Aerospace Applications; Automotive Applications; Oil/Gas Applications

Features: Chemical Resistant; Ductile; Flame Retardant; Good Dimensional Stability; Good Impact Resistance; High Heat Resistance

Printing conditions for data table:
- Filament drying conditions, minimum 4h: 150°C
- Extruder temperature: 400-440°C
- Bed temperature: 180-220°C
- Printing tool path: cross hatching in the XY plane

Test specimen parameters:
- First layer: 0.3mm thick
- Subsequent layers: 0.1mm
- 100% infill
- 3 shells
- Printing speed: 18 mm/s

Information provided by Solvay Specialty Polymers.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.29 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 48.0 MPaASTM D638
Tensile Strength, Yield 85.0 MPaASTM D638
Elongation at Break 26 %ASTM D638
Elongation at Yield 4.8 %ASTM D638
Tensile Modulus 3120 MPaASTM D638
Izod Impact, Notched 81.0 J/mASTM D256
 
Thermal PropertiesOriginal ValueComments
Melting Point 343 °C
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
ColorNatural Color
Diameter1.75 mm
FormsFilament
Processing3D Printing, Fused Filament Fabrication (FFF)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOL8Y4349 / 280149

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.