MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ceradyne SEMICORE® S1-5B MMPA 16/18 SmCo5 Samarium Cobalt Magnet  (discontinued **)
Categories: Metal; Electronic/Magnetic Alloy; Nonferrous Metal; Cobalt Alloy

Material Notes: Magnetic alignment parallel to Compaction Axis

Applications:

  • Microwave amplifiers and oscillators for airborne equipment
  • TWT modules for phased array radar
  • Small motors for severe thermal conditions
  • Hermetic magnetic couplings to replace shaft seals
  • Lightweight generators, usually for aircraft
  • Vane actuators for missiles
  • Particle beam focusing, quadrupoles, lenses, wigglers, etc.
  • Magnetic bearings, gyros, vacuum pumps, accelerometers
  • Various mechanisms in disk drives, cameras, tape drives, and miniature loudspeakers and earphones; where small size is important
  • Magnetic alignment parallel to compaction angle.

    Information provided by Ceradyne Company

    Ceradyne was acquired by 3M in 2012. The product line has been extensively renamed and reconfigured.

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesOriginal ValueComments
    Density 8.40 g/cc
     
    Electrical PropertiesOriginal ValueComments
    Electrical Resistivity 0.0000500 ohm-cm
    Magnetic Coercive Force, Hc >= 1800 OeIntrinsic
     7700 - 8300 Oe
    Magnetic Remanence, Br 8000 - 8500 Gauss
    Magnetic Maximum Energy Product, BH 16 - 18 MGOe
    Curie Temperature 700 °C
     
    Thermal PropertiesOriginal ValueComments
    CTE, linear 7.00 µm/m-°C
    @Temperature 20.0 °C
    Thermal Conductivity 0.0250 cal cm/sec-cm²-°C
     
    Descriptive Properties
    Room Temperature Compensation, RTC, %/°C-0.045

    **
    Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

    Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    Users viewing this material also viewed the following:
    Alnico® 4 (Isotropic, Cast) Hard Magnetic Alloy
    Ceradyne SEMICORE® S1-5A MMOA 20/15 SmCo5 Samarium Cobalt Magnet
    Ceradyne SEMICORE® S2-17A MMPA 24/18 Sm2 (CoFeCuZr)17 Samarium Cobalt Magnet
    Cobalt Samarium 1 Hard Magnetic Alloy
    Goodfellow Aluminum EN AC 42100

    NCERDN01 / 15866

    Master Bond adhesives

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.