MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Covestro Bayblend® T80 XG PC/ABS Blend
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced; Polycarbonate (PC)

Material Notes: (PC+ABS)-Blend; Vicat/B 120 temperature = 130 °C; excellent flow; optimized surface quality for metallization (steam treatment)

As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.14 g/ccISO 1183-1
Moisture Absorption at Equilibrium 0.20 %ISO 62, 50% RH
Water Absorption at Saturation 0.70 %ISO 62
Viscosity 190000 cP
@Shear Rate 1000 1/s,
Temperature 260 °C
melt viscosity; b.o. ISO 11443-A
Linear Mold Shrinkage, Flow 0.0055 - 0.0075 cm/cm
@Thickness 3.00 mm
150x105x3mm; b.o. ISO 2577
Linear Mold Shrinkage, Transverse 0.0055 - 0.0075 cm/cm
@Thickness 3.00 mm
150x105x3mm; b.o. ISO 2577
Melt Flow 31 g/10 min
@Load 5.00 kg,
Temperature 260 °C
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 50.0 MPa50 mm/min; ISO 527-1,-2
Tensile Strength, Yield 62.0 MPa50 mm/min; ISO 527-1,-2
Elongation at Break >= 50 %50 mm/min; b.o. ISO 527-1,-2
Elongation at Yield 4.7 %50 mm/min; ISO 527-1,-2
Tensile Modulus 2500 MPa1 mm/min; ISO 527-1,-2
Izod Impact, Notched (ISO) 14.0 kJ/m²
@Temperature -30.0 °C
ISO 180-A
 42.0 kJ/m²
@Temperature 23.0 °C
ISO 180-A
Izod Impact, Unnotched (ISO) NB
@Temperature 23.0 °C
ISO 180-U
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+16 ohm-cmIEC 60093
Surface Resistance 1.00e+17 ohmIEC 60093
Dielectric Strength 45.0 kV/mm
@Thickness 1.00 mm
IEC 60243-1
Comparative Tracking Index 175 VSolution A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 72.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1,-2
CTE, linear, Transverse to Flow 72.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1,-2
Deflection Temperature at 0.46 MPa (66 psi) 127 °CISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi) 108 °CISO 75-1,-2
Vicat Softening Point 128 °C
@Load 5.10 kg
50°C/h; ISO 306
 130 °C
@Load 5.10 kg
120°C/h; ISO 306
Flammability, UL94 HB
@Thickness 0.850 mm
 
Processing PropertiesOriginal ValueComments
Melt Temperature 260 °CInjection molding; ISO 294
Mold Temperature 80.0 °CInjection molding; ISO 294
Injection Velocity 240 mm/secISO 294

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Zytel® ST801 NC010A PA66-HI
RTP Company RTP 300 TFE 5 Polycarbonate (PC), PTFE Lubricated
Kolon KOPA® KN133G15 G/F Reinforced Nylon 6
Polykemi AB POLYblend 65H MA5 PC/ABS-blend, Low Friction
Celanese Zytel® 70G13L NC010 PA66-GF13

PB09689 / 150821

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.