MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Henkel Loctite® Stycast® 82 SIRSW1 Two-Component Silicone Syntactic Foam
Categories: Polymer; Thermoset; Silicone; Silicone Foam

Material Notes: Product Benefits

  • Lightweight
  • Ease of use
  • Low thermal conductivity
  • High temperature resistance
  • Non-corrosive
  • Can be cured in thick sections

Cure: Heat cure

Application: Assembly

Typical Assembly Applications: Bonding lightweight molded parts and thermal barriers for aerospace applications

Loctite Stycast 82 SIRSW1 is a lightweight syntactic foam designed for aerospace applications requiring high strength, high elongation and lightweight. The special microballoons used in this system allows this material to withstand high compressive loads and make it suitable for processing in moderate shear machinery.

Information provided by Henkel.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 2.35 cPPart B
 240 cP
 375 cPPart A
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 60
Tensile Strength 1.85 MPa
Elongation at Break 157.5 %
Adhesive Bond Strength >= 1.00 MPaTensile Lap Shear Strength
 
Thermal PropertiesOriginal ValueComments
CTE, linear 185 µm/m-°C
Thermal Conductivity 0.163 W/m-K
 
Processing PropertiesOriginal ValueComments
Cure Time 2.25 hour
@Temperature 150 °C
Post Cure: 1 hour @ 200°C
Pot Life 240 min
Shelf Life 6.00 Month
@Temperature 18.0 - 25.0 °C
From date of manufacture
 
Descriptive Properties
Dry heat Resistance, Shore A (maximum)65
Weight Loss (%)< 4Cured

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHENK7906 / 255395

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.