MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Synfoam® MW-44 Syntactic Foam
Categories: Polymer; Thermoset

Material Notes: Prec-cast. SynFoam MW is a moderate cost, high performance syntactic foam designed for the most critical deep water applications. SynFoam MW has an excellent strength to weight ratio and a better cost/performance benefit than SynFoam DW. MW is typically chosen for use where cost rather than density is the primary factor in selection of syntactic foam for deep water applications. MW is offered in densities between 30 and 44 pounds per cubic foot and provides the performance necessary for standard 5K and 6K ROV's as well as other underwater vehicles where a high strength is required. SynFoam MW is available as 6” x 12” x 24” fully cured blocks. The blocks may be further machined into different sizes and shapes by the end user to meet the necessary specific tolerances and requirements. Our syntactic foam is easily bonded together with the use of our syntactic adhesive to form large structures.

Information provided by Synfoam®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 42.0 - 46.0 lb/ft³
Moisture Absorption <= 3.00 %24 hours @ depth
 
Mechanical PropertiesOriginal ValueComments
Compressive Strength 16500 psi
Compressive Modulus 320000 psi
Hydrostatic Design Basis 21500 psi
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 140 °C
 
Descriptive Properties
Depth Rating (m)11580
Service Pressure (psi)17300

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSYNF020 / 192895

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.