MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Zircar Refractory Composites RS-ZFELT Zirconia Felt
Categories: Ceramic; Oxide; Zirconium Oxide

Material Notes: ZRCI Zirconium Oxide Coating Type RS-ZIRGUARD is a cream colored, water based paint of Zirconium Oxide (ZrO2). It is produced using high-purity, partially stabilized Zirconium Oxide (4 wt% CaO). It provides a high purity ceramic coating with utility to 1900°C (3452°F). It exhibits high chemical resistance and excellent release properties. Type RS-ZIRGUARD produces a hard, abrasion and chemical resistant coating that protects all ceramic bodies against most molten metals and corrosive environments, protecting them from spalling, dusting, and chemical attack. Type RS-ZIRGUARD may be applied to soft or fibrous structures to produce a more wear resistant surface layer which is also resistant to most high temperature reactions which may degrade the ceramic.

Information provided by ZIRCAR Refractory Composites, Inc. (ZRCI)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.240 g/cc
Porosity 96 %Bulk
Vapor Pressure 8.00e-12 torr
@Temperature 1370 °C
 
Mechanical PropertiesOriginal ValueComments
Tear Strength 0.600 pli'tensile strength'
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 0.130 BTU/lb-°F
@Temperature 93.0 °C
 0.180 BTU/lb-°F
@Temperature 2371 °C
Melting Point 2593 °C
Maximum Service Temperature, Air >= 2000 °C
Shrinkage 5 %
@Temperature 1650 °C,
Time 3600 sec
Linear; Isothermal Soak
 
Component Elements PropertiesOriginal ValueComments
Al2O3 <= 0.01 %
SiO2 <= 0.02 %
Y2O3 10 %
ZrO2 >= 89 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DWA 6091/SiC/20p-T6 Aluminum SiC Metal-Matrix-Composite (Al MMC)
Zircar Refractory Composites RS-99-45 Refractory Sheet
Zircar Refractory Composites RS-A3 Refractory Sheet
Zircar Refractory Composites RS-99-60 Refractory Sheet
DWA 2009/SiC/25p-T4 Aluminum SiC Metal-Matrix-Composite (Al MMC)

CZRCI48m / 217851

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.