MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Sipchem Sahara C 070BA Polypropylene, Impact Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Impact Modified; Molded/Extruded

Material Notes: Description: SAHARA C 070BA is impact copolymer with medium flow viscosity used in injection molding. This grade is characterized by a medium stiffness-impact balance at low temperature as well as a low warpage tendency. The additive formulation provides a good heat aging resistance. This product is typically used in applications that requires high resistance to temperature. This characterized with good heat aging resistance, good impact with low warpage.

Product Characteristics:
Commercial Status: Active.
Processing Method: Injection Molding
Typical applications: Battery Cases; Automotive.

Information provided by Sahara International Petrochemical Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccISO1183-1
Melt Flow 7.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 26.0 MPaISO 527-1, -2
Elongation at Break >= 50 %ISO 527-1, -2
Elongation at Yield 7.0 %ISO 527-1, -2
Tensile Modulus 1240 MPaISO 527-1, -2
Flexural Modulus 1375 MPaISO 178
Izod Impact, Notched 7.60 J/mISO 180
Charpy Impact, Notched 4.20 kJ/m²
@Temperature -20.0 °C
Type 1, Edgewise; ISO 179
 4.70 kJ/m²
@Temperature 0.000 °C
Type 1, Edgewise; ISO 179
 9.20 kJ/m²
@Temperature 23.0 °C
Type 1, Edgewise; ISO 179
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °Cunannealed; ISO 75B-1, -2
Deflection Temperature at 1.8 MPa (264 psi) 57.0 °Cunannealed; ISO 75B-1, -2
Vicat Softening Point 68.0 °CB50; ISO 306
 149 °CA50; ISO 306
Shrinkage 1.0 - 2.5 %
 
Processing PropertiesOriginal ValueComments
Processing Temperature 210 - 250 °CBarrel temperature range
Melt Temperature 240 - 260 °C
Mold Temperature 15.0 - 40.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSIPCH031 / 285344

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.