MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Parson Adhesives SONLOCK™ 3609 Retaining Compound
Categories: Polymer; Adhesive

Material Notes: SONLOK 3609 is a fast curing, medium strength anaerobic retaining compound for continuous working temperatures up to 300°F. SONLOK 3609 retaining compound is ideal for gap distances up to 0.005” diameter. Meets US Military Specification R-46082B Type I.

Applications:

  • Join rotor to shafts in fractional and subfractional horsepower motors.
  • High temperature resistance retaining compound.
  • Used for close fitting parts, rotor on shafts, bushes, pulleys and gears.
  • Excellent retaining, sealing and thread locking compound.

Information provided by Parson Adhesives, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.10 g/cc
Brookfield Viscosity 125 cPRVT Spindle 4 @ 25 rpm
 
Mechanical PropertiesOriginal ValueComments
Compressive Strength 1960 psi
@Time 1800 sec
Steel Pins & Collars; ISO 10123
 3125 psi
@Time 86400 sec
Steel Pins & Collars; ISO 10123
Shear Strength 3125 psiSteel/Steel
 
Thermal PropertiesOriginal ValueComments
CTE, linear 80.0 µm/m-°CASTM D696 K-1
Specific Heat Capacity 0.300 J/g-°C
Thermal Conductivity 0.100 W/m-KASTM C177
Maximum Service Temperature, Air 150 °C
Minimum Service Temperature, Air -55.0 °C
Flash Point >= 100 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 - 3.00 hourFunctional
 10.0 minHandling
 24.0 hourFull
Shelf Life 12.0 Month
 
Descriptive Properties
ColorGreen
CompositionMethacrylate Ester
Initial Strength Retained (%)100Acetone for 500 hrs at 22°C
 100Ethanol for 500 hrs at 22°C
 100Ethanol for 1000 hrs at 22°C
 100Motor Oil for 500 hrs at 125°C
 100Motor Oil for 1000 hrs at 125°C
 100Gasoline for 500 hrs at 22°C
 100Gasoline for 1000 hrs at 22°C
 100Break Fluid for 500 hrs at 22°C
 100Break Fluid for 1000 hrs at 22°C
 80Water/Glycol for 1000 hrs at 87°C
 90Acetone for 1000 hrs at 22°C
 90Water/Glycol for 500 hrs at 87°C
Solvent ContentNone

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPARSN002 / 186445

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.