MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
SABIC NORYL™ Resin PKN4752 Polyphenylene Ether + PS (PPE+PS) (Americas)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene + Polyphenylene Ether, Unreinforced

Material Notes: NORYL PKN4752 resin is a non-reinforced, translucent, high heat blend of polyphenylene ether (PPE) + high impact polystyrene (HIPS). This extrudable and injection moldable grade exhibits high heat resistance, dimensional stability, and appears translucent with a yellow tint in the natural color. NORYL PKN4752 resin is an excellent candidate for high performance packaging in food, electronics, and healthcare. *See NORYL PKN4752F resin for FDA food compliant version.

Features: Hydrolytic Stability,Low Creep Sensitivity,High Heat Resistance,Translucent,Low Warpage

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.08 g/ccASTM D792
Moisture Absorption 0.000 %Sheet Extrusion
Linear Mold Shrinkage, Flow 0.0060 - 0.0090 cm/cm
@Thickness 3.20 mm
SABIC method
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 73.0 MPa50 mm/min; ASTM D638
Tensile Strength, Yield 86.0 MPa50 mm/min; ASTM D638
Elongation at Break 15 %50 mm/min; ASTM D638
Elongation at Yield 6.0 %50 mm/min; ASTM D638
Tensile Modulus 3000 MPa50 mm/min; ASTM D638
Flexural Strength 136 MPayld, 2.6 mm/min, 100 mm span; ASTM D790
 144 MPayld, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2940 MPa2.6 mm/min, 100 mm span; ASTM D790
 3150 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 32.0 JASTM D256
Dart Drop, Total Energy 6.00 JASTM D3763
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 63.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
CTE, linear, Transverse to Flow 55.8 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 160 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 151 °C
@Thickness 3.20 mm
unannealed; ASTM D648
 151 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Vicat Softening Point 173 °CRate B/50; ASTM D1525
 
Processing PropertiesOriginal ValueComments
Zone 1 205 - 225 °CSheet Extrusion
Zone 2 215 - 240 °CSheet Extrusion
Zone 3 240 - 265 °CSheet Extrusion
Zone 4 240 - 265 °CSheet Extrusion
Adapter Temperature 240 - 265 °CSheet Extrusion
Die Temperature 240 - 265 °CSheet Extrusion
Melt Temperature 265 - 275 °CSheet Extrusion
Roll Temperature 105 - 120 °CRoll Stack Temp - Bottom
 105 - 120 °CRoll Stack Temp - Middle
 105 - 120 °CRoll Stack Temp - Top
Drying Temperature 70.0 - 80.0 °CSheet Extrusion
Dry Time 2.00 - 4.00 hourSheet Extrusion
 8.00 hourCumulative; Sheet Extrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH82414 / 290361

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.