MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SABIC LEXAN™ Copolymer XHT4143 Polycarbonate (PC) (Europe)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: XHT4143 is a high flow, UV stabilized, high heat polycarbonate copolymer blend with an HDT/Af of 162C. It is available in a range of opaque and limited transparent colors.

Features: High Heat Resistance

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccASTM D792
Density 1.21 g/ccISO 1183
Moisture Absorption 0.0200 %Injection Molding
 0.250 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.33 %ISO 62-1
Viscosity 24 cP
@Load 2.16 kg,
Temperature 330 °C
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0060 - 0.0095 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 25 g/10 min
@Load 2.16 kg,
Temperature 330 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 67.0 MPa50 mm/min; ISO 527
 69.0 MPa50 mm/min; ASTM D638
Tensile Strength, Yield 77.0 MPa50 mm/min; ASTM D638
 78.0 MPa50 mm/min; ISO 527
Elongation at Break 50 %50 mm/min; ASTM D638
 50 %50 mm/min; ISO 527
Elongation at Yield 7.0 %50 mm/min; ASTM D638
 7.0 %50 mm/min; ISO 527
Tensile Modulus 2730 MPa5 mm/min; ASTM D638
 2750 MPa1 mm/min; ISO 527
Flexural Strength 80.0 MPayield, 2 mm/min; ISO 178
 120 MPayld, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2600 MPa1.3 mm/min, 50 mm span; ASTM D790
 2600 MPa2 mm/min; ISO 178
Izod Impact Notched 93.0 JASTM D256
 76.0 J
@Temperature -30.0 °C
ASTM D256
Izod Impact, Notched (ISO) 10.0 kJ/m²80*10*3; ISO 180/1A
 8.00 kJ/m²
@Temperature -30.0 °C
80*10*3; ISO 180/1A
Izod Impact, Unnotched (ISO) NB80*10*3; ISO 180/1U
 NB
@Temperature -30.0 °C
80*10*3; ISO 180/1U
Charpy Impact Unnotched NBEdgew 80*10*3 sp=62mm; ISO 179/1eU
 NB
@Temperature -30.0 °C
Edgew 80*10*3 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 11.0 kJ/m²Edgew 80*10*3 sp=62mm; ISO 179/1eA
 9.00 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*3 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 72.0 JASTM D3763
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index 175 - 250 VUL 746A
Hot Wire Ignition, HWI 15 - 30 sec
@Thickness 1.50 mm
UL 746A
High Amp Arc Ignition, HAI >= 120 arcs
@Thickness 1.50 mm
UL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 60.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 60.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 60.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 60.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
Hot Ball Pressure Test 165 °CPASS; IEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 173 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
 174 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 162 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 165 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 181 °CRate B/120; ISO 306
 183 °CRate B/50; ISO 306
 183 °CRate B/50; ASTM D1525
UL RTI, Electrical 150 °CUL 746B
UL RTI, Mechanical with Impact 130 °CUL 746B
UL RTI, Mechanical without Impact 150 °CUL 746B
Flammability, UL94 HB
@Thickness >=1.50 mm
UL 94
Glow Wire Ignition Temperature 875 °C
@Thickness 3.00 mm
IEC 60695-2-13
Glow Wire Flammability Index 960 °C
@Thickness 3.00 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 295 - 310 °C
Zone 2 290 - 305 °C
Zone 3 300 - 315 °C
Melt Temperature 300 - 315 °CInjection Molding
Mold Temperature 95.0 - 130 °C
Drying Temperature 135 °CInjection Molding
Dry Time 4.00 - 6.00 hourInjection Molding
Back Pressure 0.300 - 0.700 MPa
Shot Size 40 - 60 %
Vent Depth 0.00250 - 0.00800 cm
Screw Speed 40 - 90 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH80471 / 288418

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.