Homopolymer Features: - High melt strength and superior bubble stability
- Enhances throughputs in LLDPE blends
- Superior strength and toughness
- Excellent shrink film characteristics
Additive Packages: Applications: - Industrial packaging
- Liners
- Shrink film
- Blends with LLDPE
Film properties are typical of blown film extruded on a 1.5" extruder with 3" die and 35-mil die gap at a blow up ratio of 2.5:1, but are dependent upon operating conditions. United States: NOVAPOL LF-Y320 Series resin complies with the specifications contained in the U.S. Food and Drug Administration (FDA) regulation 21 CFR 177.1520 for olefin polymers, para. (c) 2.1, and may thus be used in the United States as an article or component of an article intended for use in contact with food. This resin is subject to the specific limitation that it may not be used in articles used for packaging or holding food during cooking. NOVA Chemicals polyethylene resins are biologically and chemically inert. Information provided by NOVA Chemicals® |