Approved vacuum insulation panel for wall application and reveals and roller blinds, with extruded polystyrene protection. Vacupor® XPS-B2-S is a Microporous insulation material which has an extremely low thermal conductivity coefficient giving it very good insulating properties. Vacupor® XPS-B2-S consists of inorganic oxides. The main constituent is fumed silica, the other components are opacifiers for minimizing infrared radiation, and fiber filaments as reinforcing fillers. Vacupor® XPS-B2-S is approved by DIBT under the certification number Z-23.11-1662.The approval is valid for construction applications DAD, DAA, DZ, DI, DEO, WAB, WAA, WH, WTR and WI according to standard DIN 4108-10, and prefabricated façade panels with insulated glass character. Vacupor® XPS-B2-S conforms to building material class E (B2). The test of behaviour in case of fire according DIN 4102-1, May 1998, building material class B2; test certificate no. H.3-145/07 and H.3-146/07, was issued by the Forschungsinstitut für Wärmeschutz e.V. München. The core material of Vacupor® XPS-B2-S is not flammable and is classified A1 according to DIN ISO EN 13501-1. Vacupor® XPS-B2-S is heat sealed in a multilayer vacuum metalised film. The very low internal pressure and the microporous panel core enable it to reach extremely low thermal conductivity values.Information provided by Morgan Advanced Materials |