MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Mocom (ALBIS) ALTECH® PBT+PC A 1000/106 PBT+PC
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced

Material Notes: Base Polymer: Polybutylene Terephthalate + Polycarbonate

Special Features: Low temperature impact modified, heat ageing stabilization

Market Segment: Injection molded parts

Application Area: Automotive, Information Technology, Electrical and Electronic

Typical Applications: Engine cover, bezels, radiator grilles, housings

Information provided by Albis Plastics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.27 g/ccISO 1183
Maximum Moisture Content 0.010
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
@Time 86400 sec
ISO 294-4
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm
@Time 86400 sec
ISO 294-4
Melt Flow 20 g/10 min
@Load 5.00 kg,
Temperature 260 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 42.0 MPaISO 527
Elongation at Break 15 %ISO 527
Tensile Modulus 1900 MPaISO 527
Flexural Strength 63.0 MPaISO 178
Flexural Modulus 1900 MPaISO 178
Charpy Impact Unnotched 70.0 kJ/m²
@Temperature -40.0 °C
ISO 179/1eU
 NB
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 3.50 kJ/m²
@Temperature -40.0 °C
ISO 179/1eA
 18.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 68.0 °CISO 75-1/-2
Vicat Softening Point 104 °CB50; ISO 306
 
Processing PropertiesOriginal ValueComments
Melt Temperature 240 - 280 °CInjection molding
Mold Temperature 80.0 - 100 °CInjection molding
Drying Temperature 100 - 105 °C
@Time 7200 - 14400 sec
in a dry air (desiccant) dryer
 100 - 105 °C
@Time 3600 - 43200 sec
air circulating dryer
 
Descriptive Properties
Base PolymerPolybutylene Terephthalate + Polycarbonate

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Makroblend® UT5205 PC/PBT Blend
Covestro Makroblend® EL 703 Polycarbonate + Polyester-based Blend, Impact Modified, Flame-Retardant, UV Stabilized
Mocom (ALBIS) ALCOM® LD PC 1000 UV 14095 GY1198-14 PC, special filler, UV stabilized
Covestro Petlon® PC/PET 36A 620UV Yellow Semi-Crystalline PET, 10% Glass Fiber
Covestro Makrolon® ET UV112 Polycarbonate

PALBIS8787 / 242846

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.