MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Ovako 19MnV6* 280T Steel, Normalizing
Categories: Metal; Ferrous Metal; Alloy Steel

Material Notes: Ovako 280T is a premium variant used in the hollow bar program of Ovako. Ovako 280T meet and is exceeding the demands of E470 in EN10294-1. Ovako 280T is a micro alloyed steel with high tensile strength, good machinability and weldability.
  • Suitable for case carburizing or nitriding
  • Good dimensional stability
  • Fine-grain treated
  • Delivered in as-rolled, normalized or quenched and tempered condition
  • Weldable if preheated
Information provided by Ovako
Key Words: 19MnVS6, E470, 20MnV6, 20 MV 6, SS 2142, 1.1301, 19MnV6
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.80 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 180
@Thickness >=25.0 mm
Tube, wall
 185
@Thickness 15.0 - 25.0 mm
Tube, wall
 190
@Thickness <=15.0 mm
Tube, wall
 200
@Thickness 24.0 - 190 mm
Round bar
 200
@Thickness 24.0 - 190 mm
Round bar
Tensile Strength 550 MPa
@Thickness 24.0 - 190 mm
Round bar
 550 MPa
@Thickness 24.0 - 190 mm
Round bar
 560 MPa
@Thickness >=25.0 mm
Tube, wall
 580 MPa
@Thickness 15.0 - 25.0 mm
Tube, wall
 600 MPa
@Thickness <=15.0 mm
Tube, wall
Tensile Strength, Yield >= 380 MPa
@Thickness >=25.0 mm
Reh, Tube, wall
 >= 400 MPa
@Thickness 15.0 - 25.0 mm
Reh, Tube, wall
 >= 410 MPa
@Thickness 24.0 - 190 mm
Reh, Round bar
 >= 410 MPa
@Thickness 24.0 - 190 mm
Reh, Round bar
 >= 430 MPa
@Thickness <=15.0 mm
Reh, Tube, wall
Elongation at Break 19 %
@Thickness 24.0 - 190 mm
Round bar
 19 %
@Thickness 24.0 - 190 mm
Round bar
 25 %
@Thickness <=15.0 mm
Tube, wall
 25 %
@Thickness 15.0 - 25.0 mm
Tube, wall
 25 %
@Thickness >=25.0 mm
Tube, wall
Modulus of Elasticity 210 GPa
Poissons Ratio 0.30
Shear Modulus 80.0 GPa
Impact Test 27.0 J
@Thickness 24.0 - 190 mm,
Temperature 20.0 °C
Round bar, long
 27.0 J
@Thickness 24.0 - 190 mm,
Temperature -40.0 °C
Round bar, long
 27.0 J
@Thickness <=15.0 mm,
Temperature -40.0 °C
Tube, wall, long
 27.0 J
@Thickness 15.0 - 25.0 mm,
Temperature -40.0 °C
Tube, wall, long
 27.0 J
@Thickness >=25.0 mm,
Temperature -40.0 °C
Tube, wall, long
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000200 - 0.00000250 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 12.0 µm/m-°C
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.460 - 0.480 J/g-°C
@Temperature 50.0 - 100 °C
Thermal Conductivity 40.0 - 45.0 W/m-KAmbient temperature
Transformation Temperature 395 °CMS
 721 °CAC1
 810 °CAC3
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.17 - 0.20 %
Chromium, Cr 0.20 - 0.28 %
Iron, Fe 96.99 - 97.78 %As Balance
Manganese, Mn 1.45 - 1.6 %
Molybdenum, Mo <= 0.10 %
Nickel, Ni <= 0.20 %
Phosphorus, P <= 0.025 %
Silicon, Si 0.30 - 0.45 %
Sulfur, S 0.020 - 0.035 %
Vanadium, V 0.080 - 0.12 %
 
Descriptive Properties
Dl1.6-1.9%
WeldabilityCEV 0.6max
 Pcm 0.35max

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

NOVAKO112 / 234411

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.