Clearflex FG 106 is a hexene copolymer linear low density polyethylene (C6-LLDPE), with antioxidants, suitable for blown film extrusion. Films manufactured with Clearflex FG 106 are characterized by excellent optical properties (haze and gloss), optimum sealing performances and high mechanical properties. Main Applications: Clearflex FG 106 is recommended for the production of agricultural film, blown stretch film coextruded or blended with LDPE. Information provided by Polimeri Europa. Versalis is the Eni subsidiary containing the plastics and rubber businesses. |