MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Thermal Ceramics Kaocrete HPM 90 Ultra High Strength Castables
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: Kaocrete HPM 90 is a 93%-alumina product designed for extremely rugged applications requiring hot strength and excellent load bearing characteristics. At 190 pcf density, Kaocrete HPM 90 is comparable to pressed high-alumina brick, with actual hot strengths at intermediate temperatures superior to a 90%-alumina brick.

Features:

  • Provide 2 to 3 times greater strengths than standard castables with similar densities
  • Superb resistance to abrasion or mechanical impact
  • Excellent thermal shock resistance
  • Resistant to slag or metal contact
  • Stronger bond formed when heated
  • Porosity rivals that of dense firebrick
  • All water used in casting is removed once monolithic reaches 350°F (177°C)
  • Information provided by Thermal Ceramics

    Data has not been recently verified. Please contact manufacturer for current information.

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesOriginal ValueComments
    Density 2.901 - 3.061 g/ccFired
    Deformation 0.60 %load-25 psi, 1.5 hours at 2640°F; ASTM C16
     
    Mechanical PropertiesOriginal ValueComments
    Modulus of Rupture 1.60 - 2.40 ksiDried 18-24 hours at 220°F; ASTM C133
     1.60 - 2.40 ksi
    @Treatment Temp. 816 °C,
    Time 18000 sec
    ASTM C133
    Compressive Strength 69.0 - 90.0 MPaDried for 18-24 hours at 220°F
     79.0 - 103 MPaFired 5 hours at 1500°F; ASTM C133
     97.0 - 124 MPaFired 5 hours at 3400°F
    Abrasion 5.0 - 8.0loss, cc`s; Fired 5 hours at 1500°F; ASTM C704
     
    Thermal PropertiesOriginal ValueComments
    Thermal Conductivity 18.5 BTU-in/hr-ft²-°F
    @Temperature 1090 °C
    ASTM C417
     20.0 BTU-in/hr-ft²-°F
    @Temperature 816 °C
    ASTM C417
     23.0 BTU-in/hr-ft²-°F
    @Temperature 538 °C
    ASTM C417
     28.3 BTU-in/hr-ft²-°F
    @Temperature 260 °C
    ASTM C417
    Maximum Service Temperature, Air 3400 °F
    Shrinkage 0.10 - 0.30 %
    @Temperature 816 °C,
    Time 18000 sec
    ASTM C113
     0.50 - 1.5 %
    @Temperature 1870 °C,
    Time 18000 sec
    ASTM C113
     0.00 - 0.20 %
    @Treatment Temp. 104 °C
    Dried 18-24 hours; ASTM C113
     
    Processing PropertiesOriginal ValueComments
    Shelf Life 12.0 Month
     
    Component Elements PropertiesOriginal ValueComments
    Al2O3 93 %
    Alkalis 0.40 %
    CaO 1.5 %
    Fe2O3 0.10 %
    SiO2 5.0 %

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    Users viewing this material also viewed the following:
    Thermal Ceramics Kaolite 3300 High Temperature Insulating Castables
    Thermal Ceramics Kaocast 3000 Dense Castable
    Morgan Advanced Ceramics Kaolite 3300 Thermal Ceramic

    CTHERM075 / 2395

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.