MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
SABIC LNP™ THERMOCOMP™ Compound DF004 Polycarbonate (PC) (Americas)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LNP THERMOCOMP DF004 compound is based on Polycarbonate (PC) resin containing 20% glass fiber.

Features: High Stiffness,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.35 g/ccASTM D792
 1.35 g/ccISO 1183
Moisture Absorption 0.0200 %Injection Molding
 0.100 %23°C/50% RH/24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.0020 cm/cm24hrs; ASTM D955
 0.0020 cm/cm24hrs; ISO 294
Linear Mold Shrinkage, Transverse 0.0045 cm/cm24hrs; ISO 294
 0.0050 cm/cm24hrs; ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 91.0 MPa5 mm/min; ASTM D638
Elongation at Break 9.5 %5 mm/min; ASTM D638
Tensile Modulus 5510 MPa50 mm/min; ASTM D638
 6000 MPa1 mm/min; ISO 527
Flexural Strength 148 MPabrk, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 5510 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 133 JASTM D256
Izod Impact, Unnotched 961 J/mASTM D4812
Izod Impact, Notched (ISO) 8.00 kJ/m²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 61.0 kJ/m²80*10*4; ISO 180/1U
 
Electrical PropertiesOriginal ValueComments
Hot Wire Ignition, HWI >= 120 sec
@Thickness >=1.50 mm
UL 746A
High Amp Arc Ignition, HAI 0.00 - 15 arcs
@Thickness >=1.50 mm
UL 746A
 30 - 60 arcs
@Thickness >=3.00 mm
UL 746A
High Voltage Arc-Tracking Rate, HVTR >= 150 mm/minUL 746A
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 144 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 142 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 139 °C
@Thickness 3.20 mm
unannealed; ASTM D648
UL RTI, Electrical 125 °CUL 746B
UL RTI, Mechanical with Impact 115 °CUL 746B
UL RTI, Mechanical without Impact 125 °CUL 746B
Flammability, UL94 V-2
@Thickness >=1.50 mm
UL 94
 V-1
@Thickness >=3.00 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Zone 2 310 - 320 °C
Zone 3 320 - 330 °C
Melt Temperature 305 - 325 °CInjection Molding
Mold Temperature 80.0 - 110 °C
Drying Temperature 120 °CInjection Molding
Dry Time 4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa
Screw Speed 30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH81511 / 289458

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.