MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Jack Pine Wood
Categories: Wood and Natural Products; Wood; Softwood

Key Words: Pinus Banksiana; Lumber, Timber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.420 g/ccGreen, based on volume
 0.430 g/cc12% moisture content, based on volume
 
Mechanical PropertiesOriginal ValueComments
Hardness, Wood Indentation 1779 NGreen
 2491 N12% moisture content
Tensile Strength at Break 360 psiGreen, perpendicular to grain
 420 psi12% moisture content, perpendicular to grain
Modulus of Elasticity 1070 ksiGreen
 1350 ksi12% moisture content
Modulus of Rupture 6.00 ksiGreen
 9.90 ksi12% moisture content
Compressive Strength 300 psiGreen, perpendicular to grain
 580 psi12% moisture content, perpendicular to grain
 2950 psiGreen, parallel to grain
 5660 psi12% moisture content, parallel to grain
Shear Strength 750 psiGreen, parallel to grain
 1170 psi12% moisture content, parallel to grain
Impact 26Impact bending in inches, green
 27Impact bending in inches, 12% moisture content
Work to Maximum Load 7.20 in-lb/in³Green
 8.30 in-lb/in³12% moisture content
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.730 BTU-in/hr-ft²-°FOven Dry, US origin
 0.890 BTU-in/hr-ft²-°F12% Moisture Content, US origin
Shrinkage 3.7 %Radial, from green to oven dry, US origin
 6.6 %Tangential, from green to oven dry, US origin
 10.3 %Volumetric, from green to oven dry, US origin

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
American Red Spruce Wood
Lodgepole Pine Wood
American Balsam Fir Wood
Red Pine Wood
American Ponderosa Pine Wood

PTSU008 / 71450

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.