MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Lanxess Addocat® 102 PU Catalyst/Activator
Categories: Other Engineering Material; Catalyst/Initiator

Material Notes: In rigid foams Addocat 102 catalyses mainly the crosslinking reaction (isocyanate-polyol). For the production of these materials Addocat 102 is used as a co-catalyst in combination with Addocat 726 b, Addocat 104 or Addocat PP. It gives the rigid foam a tough and elastic skin, thus improving the adhesion of the foam to facings, particularly in sandwich panels.

Function: Catalyst for the production of rigid polyurethane foam.

Applications:

  • Continuous production of sandwich panels.
  • Discontinuous heat/cold insulation of refrigerators and piping.
  • On-site casting.

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.03 g/cc
Water Absorption <= 0.50 %
Viscosity 2.0 cP
 
Thermal PropertiesOriginal ValueComments
Solidus -2.00 °C
Boiling Point 198 °C
Flash Point 92.0 °CASTM D93, DIN EN 22719
 
Processing PropertiesOriginal ValueComments
Shelf Life 6.00 Month
@Temperature 20.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Baybond® PU 406 Polyurethane
Covestro Baybond® PU 330 Polyester Urethane Polymer
Ensinger Hydex™ 202 Rigid Polyurethane (PU)
Ensinger Hydex™ 301 Rigid Polyurethane (PU)
Lanxess Addocat® 104 PU Catalyst/Activator

PLANY8178 / 208571

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.