MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
SABIC NORYL GTX™ Resin GTX9400W Polyphenylene Ether + PA (PPE+Nylon) (Asia)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Polyphenylene Ether/PPO

Material Notes: NORYL GTX™ 9400W resin is a non-reinforced alloy of Polyphenylene Ether (PPE) + Polyamide (PA) that exhibits high heat resistance, high flow, and added mold release. NORYL GTX9400W resin is injection moldable and an excellent candidate for automotive under-the-hood applications such as power distribution boxes, relay boxes, connectors, sensors, and fuse box covers.

Features: Hydrolytic Stability,Chemical Resistance,Low Creep Sensitivity,Good Stiffness,Low Warpage,High Flow,Good Processability

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.10 g/ccASTM D792
Moisture Absorption 0.0700 %Injection Molding
Linear Mold Shrinkage, Flow 0.012 - 0.014 cm/cm
@Thickness 3.20 mm
SABIC method
Linear Mold Shrinkage, Transverse 0.011 - 0.014 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 97 g/10 min
@Load 5.00 kg,
Temperature 280 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 62.0 MPa50 mm/min; ASTM D638
Tensile Strength, Yield 64.0 MPa50 mm/min; ASTM D638
 69.0 MPa50 mm/min; ISO 527
Elongation at Break 39 %5 mm/min; ISO 527
 40 %50 mm/min; ASTM D638
Elongation at Yield 11 %50 mm/min; ASTM D638
Tensile Modulus 1950 MPa50 mm/min; ASTM D638
Flexural Strength 100 MPayld, 2.6 mm/min, 100 mm span; ASTM D790
Flexural Modulus 2350 MPa2.6 mm/min, 100 mm span; ASTM D790
 2700 MPa2 mm/min; ISO 178
Izod Impact Notched 256 JASTM D256
 112 J
@Temperature -30.0 °C
ASTM D256
Izod Impact, Unnotched 849 J/mASTM D4812
 768 J/m
@Temperature -30.0 °C
ASTM D4812
Izod Impact, Notched (ISO) 21.0 kJ/m²80*10*4; ISO 180/1A
 13.0 kJ/m²
@Temperature -40.0 °C
80*10*4; ISO 180/1A
 15.0 kJ/m²
@Temperature -20.0 °C
80*10*4; ISO 180/1A
Dart Drop, Total Energy 43.0 JASTM D3763
 15.0 J
@Temperature -30.0 °C
ASTM D3763
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 122 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
CTE, linear, Transverse to Flow 142 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 187 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
 190 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 78.0 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 83.0 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 203 °CRate B/50; ISO 306
 212 °CRate B/50; ASTM D1525
Flammability, UL94 HB
@Thickness >=1.50 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 270 - 295 °C
Zone 2 260 - 295 °C
Zone 3 265 - 295 °C
Melt Temperature 270 - 295 °CInjection Molding
Mold Temperature 65.0 - 95.0 °C
Drying Temperature 95.0 - 105 °CInjection Molding
Dry Time 3.00 - 4.00 hourInjection Molding
 8.00 hourCumulative; Injection Molding
Moisture Content 0.020 %minimum
Back Pressure 0.300 - 1.40 MPa
Shot Size 30 - 50 %
Vent Depth 0.00130 - 0.00380 cm
Screw Speed 20 - 100 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH82174 / 290121

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.